Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.223 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.084 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcm [57] |
Hall-P 2c 2b |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 328.1 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 286.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 286.3 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 1> | 259.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 187.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 234.3 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 173.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 328.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 281.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 72.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 234.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 173.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 328.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 249.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 290.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 249.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 249.4 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 173.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 259.5 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 290.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 140.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 259.5 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 86.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 249.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 110.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 286.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 290.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 110.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 328.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 218.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 218.1 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 234.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 46.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 234.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 328.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 286.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 234.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 328.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 140.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 140.6 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 249.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 328.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 234.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 140.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 328.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 218.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 234.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 290.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 249.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 328.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K3GeTe3 (mp-27331) | 0.6346 | 0.000 | 3 |
Cs3HgI5 (mp-651121) | 0.6453 | 0.002 | 3 |
Ba2CrO4 (mp-566511) | 0.6585 | 0.000 | 3 |
Rb3SbS4 (mp-17154) | 0.6492 | 0.000 | 3 |
Tl2PSe3 (mp-28394) | 0.6461 | 0.000 | 3 |
Sm2SiTeO4 (mp-6055) | 0.1282 | 0.000 | 4 |
La2SiSeO4 (mp-17834) | 0.4491 | 0.000 | 4 |
Nd2SiTeO4 (mp-18542) | 0.0469 | 0.000 | 4 |
Ce2SiTeO4 (mp-542663) | 0.0624 | 0.032 | 4 |
Gd2SiTeO4 (mp-16788) | 0.2523 | 0.020 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Si Te O |
Final Energy/Atom-7.6124 eV |
Corrected Energy-254.8350 eV
-254.8350 eV = -243.5984 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)