Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.060 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.870 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 269.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 205.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 205.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 269.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 303.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 269.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 326.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 211.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 269.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 226.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 195.8 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 163.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 79.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 326.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 224.6 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 115.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 224.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 326.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 242.8 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 316.9 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 314.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 195.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 261.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 273.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 261.0 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 302.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 273.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 68.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 226.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 314.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 273.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 179.7 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 136.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 314.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 314.4 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 269.5 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 205.3 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 211.7 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 121.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 316.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 273.7 |
MoS2 (mp-1434) | <1 1 0> | <1 1 0> | 237.6 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 68.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 303.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 316.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 182.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 326.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 130.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 182.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaGe2O5 (mp-554678) | 0.5387 | 0.014 | 3 |
Na2Mo2O5 (mp-1099875) | 0.5639 | 0.142 | 3 |
MnSi2O5 (mp-19351) | 0.3444 | 0.103 | 3 |
Na2W2O5 (mp-1076261) | 0.5798 | 0.275 | 3 |
CaGe2O5 (mp-3707) | 0.2580 | 0.006 | 3 |
CaTiSiO5 (mp-6109) | 0.2484 | 0.000 | 4 |
CaFeSiO5 (mvc-3263) | 0.2682 | 0.062 | 4 |
SrTiGeO5 (mp-559957) | 0.1907 | 0.000 | 4 |
CaTiSiO5 (mp-6440) | 0.3096 | 0.000 | 4 |
NaVAsO5 (mp-19621) | 0.2120 | 0.000 | 4 |
NaAlPO4F (mp-8678) | 0.4148 | 0.002 | 5 |
CaAlSiO4F (mp-6873) | 0.3206 | 0.029 | 5 |
NaAlAsO4F (mp-14395) | 0.3386 | 0.000 | 5 |
CaMgAsO4F (mp-558016) | 0.4921 | 0.000 | 5 |
CaMgAsO4F (mp-7035) | 0.4741 | 0.000 | 5 |
Ca6TiAl5Si6(O5F)5 (mp-695616) | 0.3528 | 0.026 | 6 |
NaCa4TaTi4(SiO5)5 (mp-694049) | 0.3488 | 0.002 | 6 |
NaCa9Ti9Nb(SiO5)10 (mp-534850) | 0.3514 | 0.000 | 6 |
Ca3TiAl2Si3O13F2 (mp-43114) | 0.3468 | 0.021 | 6 |
Ca5Ti3NbAl(SiO5)5 (mp-720340) | 0.3483 | 0.007 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Ti_pv Ge_d O |
Final Energy/Atom-7.5278 eV |
Corrected Energy-254.9355 eV
-254.9355 eV = -240.8897 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)