@article{Alonso2004, author = "Alonso, J.A. and Rivillas, F. and Martinez Lope, M.J. and Pomjakushin, V.", title = "Preparation and structural study from neutron diffraction data of R2 Mo O6 ( R= Dy, Ho, Er, Tm, Yb, Y )", journal = "Journal of Solid State Chemistry", year = "2004", volume = "177", pages = "2470-2476", ASTM_id = "JSSCBI" }