Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.550 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTm5Sb3 + Tm |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/n [86] |
HallP 4n 1n |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 298.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 298.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 149.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 74.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 105.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 298.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 211.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 298.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 224.0 |
Al (mp-134) | <1 1 0> | <1 1 0> | 211.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 149.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 224.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 211.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 298.6 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 211.2 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 298.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 149.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 166.8 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 149.3 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 74.7 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 149.2 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 105.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 74.7 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 105.6 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 105.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 211.2 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 298.6 |
Si (mp-149) | <1 0 0> | <0 0 1> | 149.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 298.6 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 105.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 74.7 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 74.7 |
C (mp-48) | <1 0 1> | <1 0 0> | 298.6 |
ZrO2 (mp-2858) | <1 1 1> | <1 0 0> | 149.3 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 298.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 149.2 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 298.6 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 224.0 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 224.0 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 298.6 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 298.6 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 74.7 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 105.6 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 298.6 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 149.3 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 298.6 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 74.7 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 105.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuTl2Pd (mp-3891) | 0.6107 | 0.000 | 3 |
LaCd2Pd (mp-12469) | 0.5928 | 0.000 | 3 |
YbIn2Rh (mp-12813) | 0.5752 | 0.000 | 3 |
NdCd2Pd (mp-1080579) | 0.6138 | 0.000 | 3 |
Fe2NiP (mp-571370) | 0.4643 | 0.000 | 3 |
Ti3Si (mp-980420) | 0.2792 | 0.018 | 2 |
Zr3P (mp-22447) | 0.2832 | 0.000 | 2 |
Hf3P (mp-504812) | 0.2886 | 0.000 | 2 |
Mn3P (mp-19884) | 0.4364 | 0.026 | 2 |
Ti3P (mp-31214) | 0.2491 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Sb |
Final Energy/Atom-4.9382 eV |
Corrected Energy-158.0218 eV
-158.0218 eV = -158.0218 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)