material

Nb4CrSe8

ID:

mp-17865

DOI:

10.17188/1192739


Tags: Chromium niobium selenide (1/4/8) - supercell

Material Details

Final Magnetic Moment
0.022 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.552 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.238 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cr2Se3 + Nb3Se4 + NbSe2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 53191 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
GaAs (mp-2534) <1 1 1> <0 0 1> 168.7
GaN (mp-804) <0 0 1> <0 0 1> 168.7
GaN (mp-804) <1 0 1> <1 1 1> 172.5
GaN (mp-804) <1 1 1> <0 0 1> 295.3
InAs (mp-20305) <1 0 0> <1 0 0> 193.1
InAs (mp-20305) <1 1 0> <0 0 1> 210.9
ZnSe (mp-1190) <1 1 1> <0 0 1> 168.7
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 168.7
BaF2 (mp-1029) <1 0 0> <1 0 0> 193.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 295.3
KCl (mp-23193) <1 1 1> <0 0 1> 295.3
KTaO3 (mp-3614) <1 0 0> <0 0 1> 337.5
KTaO3 (mp-3614) <1 1 0> <1 0 1> 210.7
CdS (mp-672) <0 0 1> <0 0 1> 295.3
CdS (mp-672) <1 0 0> <1 0 0> 289.7
BN (mp-984) <0 0 1> <0 0 1> 168.7
CdS (mp-672) <1 1 0> <0 0 1> 253.1
LiF (mp-1138) <1 1 0> <1 0 1> 210.7
Al (mp-134) <1 0 0> <0 0 1> 337.5
Al (mp-134) <1 1 0> <1 0 1> 210.7
Te2W (mp-22693) <0 1 0> <1 0 1> 105.4
CdTe (mp-406) <1 1 1> <0 0 1> 295.3
TePb (mp-19717) <1 1 1> <0 0 1> 295.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 295.3
Te2Mo (mp-602) <1 0 0> <1 0 1> 105.4
SiC (mp-7631) <0 0 1> <0 0 1> 295.3
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 168.7
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 126.5
MgO (mp-1265) <1 0 0> <0 0 1> 295.3
MgO (mp-1265) <1 1 0> <0 0 1> 210.9
MgO (mp-1265) <1 1 1> <0 0 1> 126.5
Ag (mp-124) <1 0 0> <0 0 1> 210.9
Ag (mp-124) <1 1 0> <0 0 1> 295.3
Ag (mp-124) <1 1 1> <0 0 1> 126.5
C (mp-66) <1 0 0> <0 0 1> 126.5
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 168.7
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 289.7
Mg (mp-153) <1 0 1> <0 0 1> 210.9
Mg (mp-153) <1 1 1> <0 0 1> 295.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 295.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 168.7
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 289.7
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 289.7
PbS (mp-21276) <1 0 0> <0 0 1> 210.9
PbS (mp-21276) <1 1 0> <0 0 1> 210.9
Ni (mp-23) <1 0 0> <0 0 1> 295.3
PbSe (mp-2201) <1 0 0> <1 0 0> 193.1
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 253.1
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 289.7
TiO2 (mp-2657) <0 0 1> <1 0 0> 193.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CrS8 (mp-5306) 0.6094 0.006 3
Mg4Ta2O9 (mp-17481) 0.6358 0.000 3
Mg4Nb2O9 (mp-17841) 0.6306 0.000 3
LiFeF3 (mp-777888) 0.6269 0.068 3
Mn(NbS2)4 (mp-3669) 0.6359 0.022 3
Li3Ni5OF11 (mp-766724) 0.6526 0.114 4
Li4Fe3TeO12 (mp-772725) 0.6477 0.112 4
Mg2VWO6 (mvc-5881) 0.6479 0.018 4
Mg2MoWO6 (mvc-5910) 0.6540 0.031 4
Mg2CrWO6 (mvc-5960) 0.6486 0.047 4
Sc2O3 (mp-755313) 0.6998 0.039 2
Cr3N2 (mp-1014444) 0.6628 0.155 2
V5S8 (mp-690772) 0.6994 0.000 2
Ga2O3 (mp-1243) 0.6928 0.030 2
Nb3S5 (mp-32983) 0.6478 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.7095 0.083 5
Li4Mn2TeWO12 (mp-768044) 0.7495 0.054 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Nb_pv Cr_pv Se
Final Energy/Atom
-6.5537 eV
Corrected Energy
-177.9485 eV
Uncorrected energy = -170.3965 eV Composition-based energy adjustment (-0.472 eV/atom x 16.0 atoms) = -7.5520 eV Corrected energy = -177.9485 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53191
Submitted by
User remarks:
  • Chromium niobium selenide (1/4/8) - supercell

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)