Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.956 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb3(Cu4S3)2 + RbCuSnS3 + Rb6Sn2S7 + Cu |
Band Gap0.863 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIbam [72] |
Hall-I 2 2c |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 303.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 151.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 128.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 193.3 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 227.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 298.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 193.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 128.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 193.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 303.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 322.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 303.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 227.9 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 227.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 227.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 322.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 193.3 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 199.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 151.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 64.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 322.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 193.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 193.3 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 227.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 193.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 322.1 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 298.8 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 76.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 193.3 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 76.0 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 199.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 193.3 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 227.9 |
MoS2 (mp-1434) | <1 1 1> | <0 1 0> | 227.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 193.3 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 151.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 193.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 322.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 227.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 128.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 64.4 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 199.2 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 322.1 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 99.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 128.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 303.8 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 303.8 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 151.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs2Mn3Te4 (mp-5927) | 0.4092 | 0.000 | 3 |
K2Mn3S4 (mp-29861) | 0.4096 | 0.468 | 3 |
Cs2Mn3Se4 (mp-3704) | 0.3730 | 0.000 | 3 |
Rb2Mn3Se4 (mp-4052) | 0.3345 | 0.000 | 3 |
Cs2Cd3Te4 (mp-567386) | 0.4053 | 0.000 | 3 |
Rb2Ti(CuS2)2 (mp-7129) | 0.5512 | 0.000 | 4 |
Tl2Cu2SnS4 (mp-18240) | 0.2096 | 0.028 | 4 |
Ba2Li3TaN4 (mp-573677) | 0.6085 | 0.008 | 4 |
K2Ag2SnSe4 (mp-570887) | 0.6121 | 0.000 | 4 |
Cs2Ti(AgS2)2 (mp-10488) | 0.5633 | 0.000 | 4 |
Ti4H3 (mp-1078123) | 0.7415 | 0.041 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Cu_pv Sn_d S |
Final Energy/Atom-4.0722 eV |
Corrected Energy-77.3236 eV
Uncorrected energy = -73.2996 eV
Composition-based energy adjustment (-0.503 eV/atom x 8.0 atoms) = -4.0240 eV
Corrected energy = -77.3236 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)