Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.177 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 138.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 232.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 116.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 223.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 210.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 149.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 297.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 149.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 210.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 223.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 105.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 297.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 210.6 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 223.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 210.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 223.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 138.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 232.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 210.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 232.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 116.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 297.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 223.4 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 116.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 232.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 232.8 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 116.4 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 1> | 138.2 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 1> | 138.2 |
C (mp-48) | <1 1 1> | <1 0 0> | 297.9 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 223.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 223.4 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 74.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 74.5 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 105.3 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 223.4 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 210.6 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 116.4 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 223.4 |
SiC (mp-11714) | <1 1 1> | <1 0 0> | 223.4 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 223.4 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 116.4 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 232.8 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 116.4 |
TiO2 (mp-390) | <1 1 1> | <1 0 0> | 223.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 223.4 |
ZnO (mp-2133) | <1 0 0> | <1 0 1> | 138.2 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 297.9 |
GaTe (mp-542812) | <1 0 0> | <1 0 1> | 138.2 |
Fe2O3 (mp-24972) | <1 0 0> | <1 1 0> | 210.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NdAl2Cu9 (mp-973410) | 0.1610 | 0.000 | 3 |
ThCo9Si2 (mp-17474) | 0.1292 | 0.025 | 3 |
SmCo9Si2 (mp-17623) | 0.1189 | 0.074 | 3 |
Ce2(Al5Ru)3 (mp-567554) | 0.7416 | 0.000 | 3 |
BaCd11 (mp-31216) | 0.1206 | 0.000 | 2 |
CaZn11 (mp-18567) | 0.0822 | 0.000 | 2 |
PrZn11 (mp-568148) | 0.0994 | 0.000 | 2 |
NdZn11 (mp-30802) | 0.1025 | 0.000 | 2 |
LaZn11 (mp-571191) | 0.0905 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Zn |
Final Energy/Atom-1.4719 eV |
Corrected Energy-35.3268 eV
-35.3268 eV = -35.3268 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)