Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.177 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.623 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4m2 [119] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 202.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 95.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 283.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 285.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 40.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 283.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 134.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 283.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 202.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 40.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 283.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 323.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 285.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 40.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 283.0 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 134.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 323.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 202.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 80.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 202.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 202.2 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 103.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 202.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 283.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 190.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 161.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 202.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 283.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 121.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 95.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 202.2 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 95.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 323.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 283.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 80.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 161.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 323.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 202.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 161.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 103.4 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 285.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 202.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 323.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 323.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 161.7 |
C (mp-66) | <1 1 1> | <1 1 0> | 134.6 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 323.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.04253 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.04253 | 0.00000 | 0.00000 |
0.06877 | -0.06877 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.09726 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
40.93 | 0.00 | 0.00 |
0.00 | 40.93 | -0.00 |
0.00 | -0.00 | 30.53 |
Dielectric Tensor εij (total) |
||
---|---|---|
47.85 | 0.00 | 0.00 |
0.00 | 47.85 | -0.00 |
0.00 | -0.00 | 35.13 |
Polycrystalline dielectric constant
εpoly∞
37.47
|
Polycrystalline dielectric constant
εpoly
43.61
|
Refractive Index n6.12 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Ga_d |
Final Energy/Atom-2.7253 eV |
Corrected Energy-32.7041 eV
-32.7041 eV = -32.7041 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)