Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.057 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 293.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 293.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 165.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 165.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 293.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 293.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 165.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 293.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 165.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 293.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 97.9 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 165.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 293.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 165.8 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 293.6 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 165.8 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 165.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 293.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 293.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 293.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 165.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 293.6 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 293.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 165.8 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 165.8 |
Si (mp-149) | <1 0 0> | <0 0 1> | 293.6 |
Si (mp-149) | <1 1 0> | <1 0 0> | 165.8 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 165.8 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 165.8 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 293.6 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 97.9 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 1> | 192.6 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 97.9 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 293.6 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 293.6 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 165.8 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 195.7 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 165.8 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 293.6 |
GaTe (mp-542812) | <1 1 0> | <1 0 1> | 192.6 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 165.8 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 293.6 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 165.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm2Cr2Fe15 (mp-3890) | 0.5742 | 0.044 | 3 |
Nd2Zn15Ge2 (mp-542178) | 0.4479 | 0.041 | 3 |
Ce2Al2Co15 (mp-16484) | 0.6806 | 0.044 | 3 |
La2Zn17 (mp-30709) | 0.2041 | 0.000 | 2 |
Tb2Fe17 (mp-571149) | 0.2158 | 0.020 | 2 |
Zr2Be17 (mp-2544) | 0.1923 | 0.000 | 2 |
Sm2Fe17 (mp-1426) | 0.2132 | 0.023 | 2 |
Ti2Be17 (mp-12648) | 0.1718 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Mg_pv |
Final Energy/Atom-1.6904 eV |
Corrected Energy-32.1183 eV
-32.1183 eV = -32.1183 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)