Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.255 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiSe2 + HgSe |
Band Gap0.145 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <0 0 1> | <1 0 0> | 201.0 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 201.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 100.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 100.5 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 201.0 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 115.4 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 201.0 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 201.0 |
Al (mp-134) | <1 1 1> | <1 0 0> | 201.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 100.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 201.0 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 230.8 |
SiC (mp-7631) | <1 0 1> | <1 0 -1> | 230.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 201.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 100.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 0> | 201.0 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 100.5 |
C (mp-66) | <1 1 1> | <1 0 0> | 201.0 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 201.0 |
Si (mp-149) | <1 1 1> | <1 0 0> | 100.5 |
C (mp-48) | <1 0 0> | <1 0 -1> | 115.4 |
C (mp-48) | <1 1 0> | <1 0 0> | 100.5 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 201.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 201.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 -1> | 230.8 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 201.0 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 1> | 165.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 -1> | 230.8 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 201.0 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 201.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 1 0> | 163.8 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 115.4 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 163.8 |
TiO2 (mp-390) | <0 0 1> | <1 0 -1> | 115.4 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 100.8 |
ZnTe (mp-2176) | <1 1 1> | <1 0 0> | 201.0 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 201.0 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 201.0 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 1> | 165.0 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 201.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd4GeS6 (mp-5151) | 0.1671 | 0.012 | 3 |
Cd4SiSe6 (mp-17791) | 0.1411 | 0.013 | 3 |
Si(Hg2S3)2 (mp-17948) | 0.1774 | 0.013 | 3 |
Cd4GeSe6 (mp-18163) | 0.1481 | 0.018 | 3 |
Cd4SiS6 (mp-18179) | 0.2189 | 0.007 | 3 |
In2Si(AgSe3)2 (mp-640614) | 0.1704 | 0.009 | 4 |
In2Cu2SiS6 (mp-558055) | 0.2817 | 0.055 | 4 |
In2Si(AgS3)2 (mp-558407) | 0.2897 | 0.006 | 4 |
In2Ag2GeSe6 (mp-505607) | 0.2756 | 0.018 | 4 |
In2Ag2GeS6 (mp-560386) | 0.3268 | 0.010 | 4 |
Si19Te8 (mp-31135) | 0.6747 | 0.036 | 2 |
GeAs2 (mp-17524) | 0.7349 | 0.000 | 2 |
Ag3P11 (mp-27821) | 0.7440 | 0.000 | 2 |
CuP10 (mp-606644) | 0.7311 | 0.000 | 2 |
Cr3N4 (mp-1015065) | 0.7483 | 0.387 | 2 |
Sr2AlCr2GaO7 (mvc-312) | 0.7174 | 0.186 | 5 |
Li2PWO4F (mp-25728) | 0.6683 | 0.352 | 5 |
LiCaMgSiN3 (mp-1020108) | 0.7424 | 0.000 | 5 |
Si (mp-644693) | 0.6992 | 0.412 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Hg Se |
Final Energy/Atom-2.7658 eV |
Corrected Energy-60.8471 eV
-60.8471 eV = -60.8471 eV (uncorrected energy)
|