material

Fe7C3

ID:

mp-18257

DOI:

10.17188/1193013


Tags: Iron carbide (7/3) Iron carbide (7/3) - h High pressure experimental phase

Material Details

Final Magnetic Moment
11.552 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
0.080 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.080 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
C + Fe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 76830 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 1 1> <0 0 1> 0.014 121.0
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.014 337.5
C (mp-48) <1 1 1> <1 0 0> 0.015 337.5
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.016 282.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.030 121.0
KCl (mp-23193) <1 1 1> <1 1 0> 0.037 212.6
KCl (mp-23193) <1 0 0> <1 0 0> 0.038 122.7
C (mp-66) <1 0 0> <1 0 0> 0.038 153.4
C (mp-48) <0 0 1> <1 0 0> 0.039 214.8
Al (mp-134) <1 0 0> <1 0 0> 0.047 245.4
InP (mp-20351) <1 1 0> <1 1 1> 0.047 200.2
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.058 121.0
BN (mp-984) <1 0 0> <1 0 1> 0.059 253.4
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.059 161.4
CdS (mp-672) <1 0 0> <1 0 1> 0.062 202.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.065 245.4
CdWO4 (mp-19387) <0 1 0> <1 1 1> 0.067 133.4
Ag (mp-124) <1 1 1> <0 0 1> 0.068 121.0
C (mp-48) <1 0 1> <1 1 1> 0.072 200.2
TeO2 (mp-2125) <0 1 0> <1 0 0> 0.072 276.1
AlN (mp-661) <1 0 0> <1 0 1> 0.073 202.8
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.079 245.4
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.104 337.5
Al (mp-134) <1 1 1> <1 0 0> 0.120 337.5
Mg (mp-153) <1 0 0> <1 0 0> 0.125 214.8
Ga2O3 (mp-886) <0 1 0> <0 0 1> 0.129 282.4
AlN (mp-661) <1 1 1> <1 0 0> 0.132 337.5
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.153 337.5
Fe2O3 (mp-24972) <1 1 0> <1 0 0> 0.156 122.7
SiC (mp-7631) <0 0 1> <1 0 0> 0.161 92.0
GaSe (mp-1943) <1 0 1> <1 0 0> 0.163 276.1
SiC (mp-11714) <0 0 1> <1 0 0> 0.168 92.0
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.171 245.4
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.177 337.5
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.183 276.1
ZnO (mp-2133) <1 1 1> <1 0 1> 0.184 253.4
Au (mp-81) <1 0 0> <0 0 1> 0.189 282.4
DyScO3 (mp-31120) <1 1 1> <1 1 0> 0.192 212.6
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.208 245.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.213 282.4
DyScO3 (mp-31120) <0 1 0> <1 0 1> 0.218 304.1
GaSe (mp-1943) <0 0 1> <0 0 1> 0.221 161.4
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.221 282.4
AlN (mp-661) <0 0 1> <1 0 0> 0.233 92.0
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.235 265.7
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.243 245.4
Au (mp-81) <1 1 0> <1 1 1> 0.245 200.2
Cu (mp-30) <1 1 1> <0 0 1> 0.246 161.4
Mg (mp-153) <0 0 1> <1 0 0> 0.261 337.5
C (mp-66) <1 1 0> <1 0 1> 0.263 304.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
373 189 179 0 0 3
189 373 179 0 0 -3
179 179 337 0 0 0
0 0 0 94 0 0
0 0 0 0 94 0
3 -3 0 0 0 92
Compliance Tensor Sij (10-12Pa-1)
4.1 -1.4 -1.4 0 0 -0.2
-1.4 4.1 -1.4 0 0 0.2
-1.4 -1.4 4.5 0 0 0
0 0 0 10.6 0 0
0 0 0 0 10.6 0
-0.2 0.2 0 0 0 10.9
Shear Modulus GV
92 GPa
Bulk Modulus KV
242 GPa
Shear Modulus GR
92 GPa
Bulk Modulus KR
241 GPa
Shear Modulus GVRH
92 GPa
Bulk Modulus KVRH
242 GPa
Elastic Anisotropy
0.01
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ta3SBr7 (mp-31015) 0.7245 0.005 3
Nb3SBr7 (mp-29057) 0.6953 0.000 3
Er7Rh3 (mp-30612) 0.4396 0.000 2
Sr7Au3 (mp-30422) 0.2775 0.000 2
B3Ru7 (mp-17535) 0.2536 0.028 2
Th7Ni3 (mp-30809) 0.4960 0.000 2
Tc7B3 (mp-978989) 0.2709 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Fe_pv C
Final Energy/Atom
-8.6172 eV
Corrected Energy
-172.3443 eV
Uncorrected energy = -172.3443 eV Corrected energy = -172.3443 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 167345
  • 76830
  • 187139
Submitted by
User remarks:
  • Iron carbide (7/3) - h

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)