Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.463 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.128 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmn21 [31] |
HallP 2ac 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 123.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 174.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 123.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 247.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 233.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 288.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 288.2 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 288.2 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 117.0 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 261.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 233.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 311.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 174.6 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 129.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 123.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 233.8 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 123.7 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 234.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 233.8 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 259.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 311.8 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 96.1 |
BN (mp-984) | <1 0 1> | <1 1 0> | 259.6 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 96.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 288.2 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 288.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 155.9 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 259.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 155.9 |
Al (mp-134) | <1 0 0> | <1 0 1> | 247.4 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 123.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 233.8 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 233.8 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 288.2 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 155.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 261.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 87.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 234.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 288.2 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 96.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 234.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 288.2 |
WS2 (mp-224) | <1 1 0> | <0 1 1> | 234.1 |
C (mp-48) | <1 1 0> | <0 1 0> | 261.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 288.2 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 288.2 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 1> | 117.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 288.2 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 1 0> | 129.8 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 192.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.09333 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.08772 | 0.00000 | 0.00000 |
0.07366 | -0.09661 | -0.21050 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.24304 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.07 | 0.00 | 0.00 |
0.00 | 6.22 | 0.00 |
0.00 | 0.00 | 6.02 |
Dielectric Tensor εij (total) |
||
---|---|---|
12.27 | 0.00 | 0.00 |
0.00 | 13.69 | 0.00 |
0.00 | 0.00 | 13.04 |
Polycrystalline dielectric constant
εpoly∞
6.10
|
Polycrystalline dielectric constant
εpoly
13.00
|
Refractive Index n2.47 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K7TaAs4 (mp-18073) | 0.0249 | 0.000 | 3 |
Rb7NbAs4 (mp-18440) | 0.1714 | 0.000 | 3 |
K5GaSe4 (mp-29377) | 0.6631 | 0.000 | 3 |
Cs2HgBr4 (mp-619546) | 0.6116 | 0.006 | 3 |
Cs2CdI4 (mp-568134) | 0.5848 | 0.011 | 3 |
RbBaTaS4 (mp-863024) | 0.6781 | 0.000 | 4 |
Na3Sr3AlP4 (mp-41095) | 0.6810 | 0.000 | 4 |
Sm3Si2S8Br (mp-555527) | 0.6973 | 0.000 | 4 |
K4Sr2SnAs4 (mp-570311) | 0.6430 | 0.000 | 4 |
Na3Sr3GaP4 (mp-10096) | 0.6975 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Nb_pv As |
Final Energy/Atom-3.5059 eV |
Corrected Energy-84.1413 eV
-84.1413 eV = -84.1413 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)