Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.116 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.311 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnnm [58] |
Hall-P 2 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 346.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 178.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 178.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 197.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 197.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 346.3 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 154.6 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 231.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 197.9 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 296.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 346.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 247.4 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 296.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 247.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 118.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 49.5 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 197.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 346.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 346.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 99.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 197.9 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 178.1 |
Al (mp-134) | <1 1 0> | <0 1 1> | 231.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 197.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 346.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 148.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 237.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 346.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 247.4 |
CdTe (mp-406) | <1 1 1> | <0 1 0> | 296.8 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 148.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 148.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 296.8 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 237.4 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 237.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 296.8 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 247.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 237.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 178.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 237.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 178.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 197.9 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 237.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 346.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 247.4 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 346.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 346.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 178.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 197.9 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 346.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La3LuSe6 (mp-645695) | 0.2204 | 0.000 | 3 |
Ce3LuSe6 (mp-645694) | 0.2598 | 0.000 | 3 |
Pr3InSe6 (mp-21575) | 0.2637 | 0.000 | 3 |
Tb3CrSe6 (mp-505638) | 0.0575 | 0.110 | 3 |
Sm3CrSe6 (mp-10386) | 0.1206 | 0.050 | 3 |
KSm2Sb3Se8 (mp-567322) | 0.5816 | 0.005 | 4 |
Tb8CrTe13Cl (mp-570277) | 0.4482 | 0.066 | 4 |
Sm8CrTe13Cl (mp-680161) | 0.4717 | 0.040 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Cr_pv S |
Final Energy/Atom-6.5354 eV |
Corrected Energy-273.4893 eV
Uncorrected energy = -261.4173 eV
Composition-based energy adjustment (-0.503 eV/atom x 24.0 atoms) = -12.0720 eV
Corrected energy = -273.4893 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)