Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.416 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.768 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmn21 [31] |
HallP 2ac 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 253.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 253.9 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 253.9 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 284.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 141.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 208.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 169.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 284.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 94.8 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 284.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 284.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 104.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 169.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 254.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 208.6 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 141.0 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 208.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 284.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 253.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 208.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 141.0 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 253.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 253.9 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 284.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 189.7 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 104.3 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 169.3 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 208.6 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 141.0 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 1 0> | 141.0 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 1 0> | 141.0 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 104.3 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 169.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 104.3 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 284.5 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 208.6 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 253.9 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 104.3 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 208.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 84.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 254.2 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 208.6 |
WS2 (mp-224) | <1 0 0> | <1 0 1> | 134.3 |
NaCl (mp-22862) | <1 1 0> | <1 0 1> | 134.3 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 284.5 |
WS2 (mp-224) | <0 0 1> | <1 1 0> | 141.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 84.6 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 284.5 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 284.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 253.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KLa(PS3)2 (mp-560649) | 0.6144 | 0.000 | 4 |
KLa(PSe3)2 (mp-571662) | 0.5315 | 0.000 | 4 |
K6NbAs3O (mp-561202) | 0.6055 | 0.000 | 4 |
K8NbAs5Pb (mp-567424) | 0.5640 | 0.000 | 4 |
K2Th(PSe3)3 (mp-568203) | 0.6236 | 0.000 | 4 |
NaSn5 (mp-31284) | 0.7131 | 0.009 | 2 |
K7TaAs4 (mp-18073) | 0.2034 | 0.000 | 3 |
K7NbAs4 (mp-18361) | 0.1974 | 0.000 | 3 |
K5GaSe4 (mp-29377) | 0.5927 | 0.000 | 3 |
K2MoS4 (mp-17980) | 0.5931 | 0.000 | 3 |
K2WSe4 (mp-18138) | 0.5357 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points8 |
U Values-- |
PseudopotentialsVASP PAW: As Rb_sv Nb_pv |
Final Energy/Atom-3.3752 eV |
Corrected Energy-81.0039 eV
-81.0039 eV = -81.0039 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)