Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.674 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa2Si2O7 |
Band Gap4.554 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 239.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 334.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 239.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 239.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 334.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 334.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 286.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 173.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 239.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 334.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 284.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 296.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 284.2 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 189.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 262.3 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 284.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 243.6 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 284.2 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 253.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 334.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 191.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 334.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 174.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 239.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 262.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 286.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 239.1 |
Al (mp-134) | <1 1 0> | <1 0 1> | 296.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 286.9 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 239.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 284.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 239.1 |
Al (mp-134) | <1 1 1> | <0 1 1> | 284.2 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 239.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 191.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 262.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 -1> | 207.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 174.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 334.7 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 284.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 239.1 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 260.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 334.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 286.9 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 239.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 334.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 239.1 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 243.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 239.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 286.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce2Si2O7 (mp-672208) | 0.2200 | 0.003 | 3 |
Sm2Si2O7 (mp-21794) | 0.3332 | 0.026 | 3 |
Pr2Si2O7 (mp-3160) | 0.2575 | 0.008 | 3 |
La2Si2O7 (mp-5974) | 0.2521 | 0.009 | 3 |
Nd2Si2O7 (mp-15225) | 0.3077 | 0.000 | 3 |
K3Bi5(AsO4)6 (mp-567022) | 0.6706 | 0.005 | 4 |
RbP3PbO9 (mp-557256) | 0.5926 | 0.000 | 4 |
K3Ga2(PO4)3 (mp-6805) | 0.6377 | 0.000 | 4 |
K5B(SO4)4 (mp-1019797) | 0.6354 | 0.000 | 4 |
BaCaP2O7 (mp-1019543) | 0.6260 | 0.002 | 4 |
Zn2Si3Pb4SO15 (mp-559184) | 0.6410 | 0.000 | 5 |
K2Cr2AsHO10 (mp-744205) | 0.7237 | 0.000 | 5 |
SrCaP2WO8 (mvc-3024) | 0.7281 | 0.266 | 5 |
SrZnP2WO8 (mvc-3145) | 0.6382 | 0.279 | 5 |
KNaLi2(SO4)2 (mp-14484) | 0.6021 | 0.000 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.7288 | 0.016 | 6 |
NaSnPHO4F (mp-766448) | 0.7190 | 0.015 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Si O |
Final Energy/Atom-8.2597 eV |
Corrected Energy-382.6621 eV
Uncorrected energy = -363.4261 eV
Composition-based energy adjustment (-0.687 eV/atom x 28.0 atoms) = -19.2360 eV
Corrected energy = -382.6621 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)