Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.566 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.114 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 186.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 110.2 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 266.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 233.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 165.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 233.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 186.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 329.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 233.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 207.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 285.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 259.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 266.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 243.6 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 121.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 220.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 326.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 220.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 55.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 258.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 285.6 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 329.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 181.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 233.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 207.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 165.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 55.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 155.8 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 302.9 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 155.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 181.7 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 258.5 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 304.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 165.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 165.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 181.7 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 258.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 311.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 186.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 181.7 |
Te2Mo (mp-602) | <1 0 1> | <1 1 -1> | 329.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 165.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 233.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 207.7 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 246.5 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 246.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 233.7 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 259.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 233.7 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 207.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaThBr6 (mp-29015) | 0.7191 | 0.053 | 3 |
SrThBr6 (mp-29016) | 0.7349 | 0.045 | 3 |
DyP5 (mp-9850) | 0.5904 | 0.003 | 2 |
PrP5 (mp-9848) | 0.5010 | 0.000 | 2 |
NdP5 (mp-7332) | 0.5164 | 0.000 | 2 |
GdP5 (mp-680742) | 0.5346 | 0.000 | 2 |
SmP5 (mp-9849) | 0.5417 | 0.000 | 2 |
TlAgAs2PbS5 (mp-677611) | 0.7361 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La P |
Final Energy/Atom-5.9002 eV |
Corrected Energy-141.6038 eV
-141.6038 eV = -141.6038 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)