material

VS

ID:

mp-1868

DOI:

10.17188/1193340


Tags: Vanadium sulfide (1/1) Vanadium(II) sulfide

Material Details

Final Magnetic Moment
0.107 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.227 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.063 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.07 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
V5S4 + V3S4
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 24564 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <1 0 0> <0 1 1> 0.007 185.3
LiGaO2 (mp-5854) <1 0 0> <0 1 1> 0.015 105.9
Bi2Te3 (mp-34202) <0 0 1> <1 0 1> 0.015 154.5
CaCO3 (mp-3953) <0 0 1> <1 0 1> 0.016 154.5
InAs (mp-20305) <1 0 0> <1 0 0> 0.019 304.4
C (mp-66) <1 1 1> <1 0 1> 0.020 154.5
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.020 93.4
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.020 270.6
LiF (mp-1138) <1 1 1> <1 0 1> 0.021 115.9
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.023 93.4
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.023 280.1
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.026 304.4
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.027 304.4
CeO2 (mp-20194) <1 1 1> <1 0 1> 0.037 154.5
C (mp-48) <1 0 0> <0 1 1> 0.038 211.7
Si (mp-149) <1 1 1> <1 0 1> 0.041 154.5
PbSe (mp-2201) <1 1 1> <1 0 1> 0.048 270.4
WSe2 (mp-1821) <1 1 0> <0 0 1> 0.050 261.5
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.051 56.0
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.053 336.2
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.056 38.6
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.057 38.6
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.063 205.4
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.072 56.0
SrTiO3 (mp-4651) <1 1 1> <0 0 1> 0.075 280.1
GaSb (mp-1156) <1 1 1> <1 0 1> 0.078 270.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.084 298.8
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.087 214.7
WS2 (mp-224) <1 0 1> <0 0 1> 0.090 93.4
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.091 56.0
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.102 135.3
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.104 93.4
CdSe (mp-2691) <1 1 1> <1 0 1> 0.110 270.4
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.111 304.4
C (mp-48) <1 1 1> <0 1 1> 0.112 238.2
SiO2 (mp-6930) <0 0 1> <1 0 1> 0.117 154.5
BaF2 (mp-1029) <1 1 1> <1 0 1> 0.121 270.4
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.138 67.6
Ni (mp-23) <1 0 0> <0 1 1> 0.144 185.3
InSb (mp-20012) <1 1 0> <0 0 1> 0.145 186.8
GaAs (mp-2534) <1 1 0> <0 0 1> 0.146 93.4
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.146 93.4
CdTe (mp-406) <1 1 0> <0 0 1> 0.148 186.8
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.151 224.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.158 33.8
SiC (mp-11714) <1 0 1> <0 0 1> 0.160 224.1
TiO2 (mp-390) <1 0 1> <0 0 1> 0.160 354.8
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.161 130.7
Al2O3 (mp-1143) <0 0 1> <0 1 1> 0.164 79.4
Ge (mp-32) <1 1 0> <0 0 1> 0.165 93.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
251 132 69 0 0 0
132 235 112 0 0 0
69 112 226 0 0 0
0 0 0 117 0 0
0 0 0 0 59 0
0 0 0 0 0 117
Compliance Tensor Sij (10-12Pa-1)
5.6 -3.1 -0.2 0 0 0
-3.1 7.2 -2.7 0 0 0
-0.2 -2.7 5.8 0 0 0
0 0 0 8.6 0 0
0 0 0 0 16.9 0
0 0 0 0 0 8.5
Shear Modulus GV
85 GPa
Bulk Modulus KV
149 GPa
Shear Modulus GR
75 GPa
Bulk Modulus KR
146 GPa
Shear Modulus GVRH
80 GPa
Bulk Modulus KVRH
147 GPa
Elastic Anisotropy
0.71
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiCoS2 (mp-753946) 0.5091 0.000 3
LiFeS2 (mp-756094) 0.5346 0.110 3
LiMoS2 (mp-30248) 0.5452 0.023 3
LiNiS2 (mp-754727) 0.5304 0.091 3
NiMoP2 (mp-10208) 0.5540 0.000 3
Li8Cr(FeO4)3 (mp-767681) 0.7385 1.300 4
Li8TiMn3O12 (mp-767679) 0.7384 0.088 4
Li8Cr3SbO12 (mp-767231) 0.7316 0.088 4
Li8MnCr3O12 (mp-766919) 0.7332 0.113 4
Li8Mn3CrO12 (mp-765119) 0.7218 0.107 4
CrAs (mp-20717) 0.3509 0.000 2
CrAs (mp-1078213) 0.3758 0.000 2
AsRu (mp-15650) 0.3738 0.036 2
MnTe (mp-1079443) 0.3035 0.179 2
TiSe (mp-571651) 0.2550 0.016 2
Si (mp-8629) 0.7357 0.292 1
N2 (mp-1061298) 0.7157 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv S
Final Energy/Atom
-7.5045 eV
Corrected Energy
-62.6899 eV
-62.6899 eV = -60.0360 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 602567
  • 651373
  • 651366
  • 24564
  • 52212
  • 41778
Submitted by
User remarks:
  • Vanadium(II) sulfide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)