Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-2.430 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTm2S3 + TmS |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 142.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 238.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 333.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 333.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 285.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 238.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 333.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 333.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 238.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 333.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 142.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 333.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 238.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 285.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 333.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 333.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 238.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 263.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 333.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 285.6 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 131.7 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 131.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 95.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 238.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 95.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 333.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 142.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 333.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 333.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 333.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 142.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 333.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 333.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 333.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 333.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 238.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 285.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 142.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 333.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 333.2 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 95.2 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 285.6 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 333.2 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 333.2 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 190.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 238.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 238.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 333.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 238.0 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 333.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KCu(BiS2)2 (mp-558063) | 0.6659 | 0.000 | 4 |
Y5S7 (mp-15670) | 0.5274 | 0.000 | 2 |
Fe3O4 (mp-715438) | 0.5539 | 0.058 | 2 |
Hf5N5O2 (mp-761032) | 0.4029 | 0.052 | 3 |
Y2CrS4 (mp-555795) | 0.5135 | 0.058 | 3 |
Hf5N5O2 (mp-761034) | 0.4635 | 0.072 | 3 |
Zr5N5O2 (mp-754891) | 0.4044 | 0.061 | 3 |
Zr5N5O2 (mp-776331) | 0.3527 | 0.051 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points24 |
U Values-- |
PseudopotentialsVASP PAW: S Tm_3 |
Final Energy/Atom-6.3218 eV |
Corrected Energy-254.8254 eV
-254.8254 eV = -240.2293 eV (uncorrected energy) - 14.5961 eV (MP Anion Correction)
|