material

YCrO3

ID:

mp-18725

DOI:

10.17188/1183675


Tags: Yttrium chromate(III) Yttrium chromate Holmium chromate(III)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-3.212 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.338 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.007 301.6
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.015 129.2
Te2Mo (mp-602) <1 0 0> <0 1 0> 0.015 163.2
CdTe (mp-406) <1 0 0> <1 0 1> 0.028 262.2
Au (mp-81) <1 0 0> <1 1 0> 0.035 296.6
InSb (mp-20012) <1 0 0> <1 0 1> 0.040 262.2
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.041 52.4
SiC (mp-11714) <1 1 1> <0 0 1> 0.049 328.7
DyScO3 (mp-31120) <1 1 0> <1 0 1> 0.056 314.6
MgF2 (mp-1249) <0 0 1> <1 0 1> 0.058 262.2
MoS2 (mp-1434) <1 0 0> <0 1 1> 0.070 202.3
GaSe (mp-1943) <0 0 1> <0 1 0> 0.070 204.0
SiC (mp-7631) <1 0 1> <1 1 0> 0.073 237.3
TiO2 (mp-2657) <0 0 1> <1 0 1> 0.074 262.2
SiC (mp-7631) <0 0 1> <0 0 1> 0.075 149.4
GaN (mp-804) <0 0 1> <0 0 1> 0.075 89.6
SiC (mp-11714) <0 0 1> <0 0 1> 0.076 149.4
Ag (mp-124) <1 0 0> <1 1 0> 0.079 296.6
Cu (mp-30) <1 0 0> <1 1 0> 0.080 118.7
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.082 119.5
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.096 344.7
SiC (mp-11714) <1 1 0> <0 1 0> 0.096 163.2
SiC (mp-7631) <1 0 0> <1 1 0> 0.103 237.3
TbScO3 (mp-31119) <1 1 0> <1 0 1> 0.104 314.6
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.104 215.4
SiC (mp-7631) <1 1 0> <0 1 0> 0.105 81.6
SiC (mp-8062) <1 1 0> <0 1 0> 0.124 81.6
C (mp-66) <1 1 0> <0 1 0> 0.127 163.2
CdSe (mp-2691) <1 1 0> <0 1 0> 0.131 163.2
ZnTe (mp-2176) <1 1 0> <0 1 0> 0.139 163.2
TePb (mp-19717) <1 0 0> <1 0 1> 0.140 262.2
GaSb (mp-1156) <1 1 0> <0 1 0> 0.146 163.2
Mg (mp-153) <1 0 0> <0 1 1> 0.147 50.6
InAs (mp-20305) <1 1 0> <0 1 0> 0.148 163.2
GaN (mp-804) <1 0 1> <0 0 1> 0.148 268.9
TeO2 (mp-2125) <0 1 0> <0 0 1> 0.154 209.2
Te2W (mp-22693) <0 1 0> <0 1 0> 0.163 163.2
AlN (mp-661) <1 0 0> <1 0 0> 0.163 172.3
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.164 258.5
SiO2 (mp-6930) <0 0 1> <0 1 0> 0.166 326.3
PbSe (mp-2201) <1 1 0> <0 1 0> 0.172 163.2
CeO2 (mp-20194) <1 1 1> <0 1 0> 0.173 204.0
AlN (mp-661) <1 1 1> <0 1 1> 0.181 202.3
BN (mp-984) <0 0 1> <0 1 1> 0.181 252.8
Si (mp-149) <1 1 1> <0 1 0> 0.183 204.0
C (mp-66) <1 0 0> <1 0 1> 0.184 314.6
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.184 258.5
Te2W (mp-22693) <0 0 1> <0 1 1> 0.187 202.3
C (mp-48) <1 1 1> <0 0 1> 0.189 268.9
NaCl (mp-22862) <1 0 0> <1 0 0> 0.192 129.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.35 0.00 0.00
0.00 5.14 0.00
0.00 0.00 5.26
Dielectric Tensor εij (total)
15.35 0.00 0.00
0.00 18.45 0.00
0.00 0.00 17.57
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.25
Polycrystalline dielectric constant εpoly
(total)
17.12
Refractive Index n
2.29
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TbCrO3 (mp-769920) 0.0501 0.158 3
HoCrO3 (mp-769818) 0.0519 0.171 3
TbFeO3 (mp-24952) 0.0403 0.001 3
DyCrO3 (mp-19381) 0.0159 0.163 3
YCrO3 (mvc-10868) 0.0212 0.000 3
Sm2MgIrO6 (mp-980108) 0.1275 0.006 4
Ca2SnIrO6 (mvc-5666) 0.1701 0.067 4
Ca2SnSbO6 (mvc-3972) 0.1732 0.076 4
Y2MnNiO6 (mp-19192) 0.1746 0.000 4
CaPr(AgO3)2 (mvc-9268) 0.1818 0.088 4
U2S3 (mp-672690) 0.6840 0.194 2
Al2O3 (mp-642363) 0.5841 0.280 2
Cr3C2 (mp-570112) 0.6144 0.030 2
Ga2O3 (mp-13134) 0.6663 0.284 2
Fe2O3 (mp-1078361) 0.6536 0.704 2
Mg11AlFeSi11O36 (mp-743592) 0.3281 0.225 5
LiLaNdSbO6 (mp-776091) 0.2984 0.006 5
LaMgCrSbO6 (mvc-9859) 0.3293 0.329 5
LaMgCrSnO6 (mvc-9925) 0.3357 0.148 5
CaLaMnRuO6 (mp-690556) 0.3270 0.080 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
700 eV
# of K-points
None
U Values
Cr: 3.7 eV
Pseudopotentials
VASP PAW: Y_sv Cr_pv O
Final Energy/Atom
-8.5802 eV
Corrected Energy
-187.8443 eV
Uncorrected energy = -171.6043 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Composition-based energy adjustment (-1.999 eV/atom x 4.0 atoms) = -7.9960 eV Corrected energy = -187.8443 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 192859
  • 109352
  • 185525
  • 236372
  • 251107
Submitted by
User remarks:
  • Yttrium chromate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)