material

CaCu5

ID:

mp-1882

DOI:

10.17188/1193525


Tags: Calcium copper (1/5)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.122 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.54 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 58882 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.000 158.0
Au (mp-81) <1 1 1> <0 0 1> 0.001 90.3
Cu (mp-30) <1 0 0> <1 0 1> 0.003 91.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.003 158.0
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.004 164.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.004 158.0
SiC (mp-11714) <0 0 1> <0 0 1> 0.005 158.0
Cu (mp-30) <1 1 1> <0 0 1> 0.005 22.6
SiC (mp-11714) <1 1 1> <1 0 0> 0.005 164.4
Ag (mp-124) <1 1 1> <0 0 1> 0.007 90.3
InP (mp-20351) <1 0 0> <1 0 1> 0.011 213.7
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.015 267.2
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.030 61.7
PbSe (mp-2201) <1 1 1> <0 0 1> 0.031 67.7
MgO (mp-1265) <1 1 0> <1 0 1> 0.033 152.7
CeO2 (mp-20194) <1 1 0> <1 0 1> 0.033 335.9
Si (mp-149) <1 1 0> <1 0 1> 0.036 335.9
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.038 67.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.038 67.7
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.041 67.7
ZnSe (mp-1190) <1 1 1> <1 1 0> 0.045 284.8
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.045 164.4
SiC (mp-11714) <1 1 0> <1 0 0> 0.052 164.4
GaSb (mp-1156) <1 1 1> <0 0 1> 0.053 67.7
Mg (mp-153) <0 0 1> <1 0 0> 0.055 226.1
Al (mp-134) <1 0 0> <1 0 0> 0.059 82.2
GaAs (mp-2534) <1 1 1> <1 1 0> 0.060 284.8
GaAs (mp-2534) <1 0 0> <1 0 0> 0.061 164.4
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.061 320.4
BN (mp-984) <1 0 1> <1 1 0> 0.063 142.4
Al2O3 (mp-1143) <1 0 0> <1 1 1> 0.063 126.5
C (mp-48) <0 0 1> <0 0 1> 0.064 67.7
C (mp-66) <1 1 0> <0 0 1> 0.066 90.3
PbS (mp-21276) <1 0 0> <1 0 1> 0.067 213.7
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.070 22.6
Te2W (mp-22693) <0 1 0> <1 0 0> 0.070 267.2
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.071 67.7
GaN (mp-804) <0 0 1> <1 1 1> 0.072 126.5
CdSe (mp-2691) <1 1 1> <0 0 1> 0.074 67.7
BaF2 (mp-1029) <1 1 0> <1 1 1> 0.077 168.6
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.082 305.3
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.095 82.2
Te2W (mp-22693) <0 0 1> <1 0 1> 0.099 244.3
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.101 308.3
Ge (mp-32) <1 1 1> <1 1 0> 0.103 284.8
Ge (mp-32) <1 0 0> <1 0 0> 0.103 164.4
GaSe (mp-1943) <1 0 0> <1 0 1> 0.103 274.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.109 226.1
WS2 (mp-224) <0 0 1> <1 0 0> 0.110 226.1
BN (mp-984) <1 1 0> <0 0 1> 0.112 67.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
127 61 71 0 0 0
61 127 71 0 0 0
71 71 169 0 0 0
0 0 0 41 0 0
0 0 0 0 41 0
0 0 0 0 0 33
Compliance Tensor Sij (10-12Pa-1)
11.4 -3.6 -3.3 0 0 0
-3.6 11.4 -3.3 0 0 0
-3.3 -3.3 8.7 0 0 0
0 0 0 24.1 0 0
0 0 0 0 24.1 0
0 0 0 0 0 30.2
Shear Modulus GV
38 GPa
Bulk Modulus KV
92 GPa
Shear Modulus GR
37 GPa
Bulk Modulus KR
90 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
91 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
UAl3Ni2 (mp-2903) 0.0400 0.105 3
CeGa3Pd2 (mp-3494) 0.0804 0.000 3
UAl3Pd2 (mp-4561) 0.0092 0.080 3
CeAl3Pd2 (mp-4785) 0.0523 0.000 3
LaGa3Pd2 (mp-21201) 0.0028 0.000 3
DyFe5 (mp-568006) 0.0067 0.000 2
CaZn5 (mp-1734) 0.0054 0.000 2
LaCo5 (mp-1731) 0.0014 0.033 2
BaPd5 (mp-2606) 0.0024 0.000 2
PrZn5 (mp-12602) 0.0028 0.008 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Cu_pv
Final Energy/Atom
-3.8722 eV
Corrected Energy
-23.2333 eV
Uncorrected energy = -23.2333 eV Corrected energy = -23.2333 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 619214
  • 184363
  • 58883
  • 619215
  • 58882
  • 260679
Submitted by
User remarks:
  • Calcium copper (1/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)