material

SnTe

ID:

mp-1883

DOI:

10.17188/1193534


Tags: Tin telluride (1/1) Tin telluride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.497 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.19 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.662 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 52489 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 1 0> <1 1 0> 0.000 174.7
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.000 164.7
BN (mp-984) <0 0 1> <1 1 1> 0.006 71.3
GaAs (mp-2534) <1 0 0> <1 0 0> 0.008 164.7
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.015 285.3
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.018 116.5
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.019 71.3
KCl (mp-23193) <1 1 1> <1 1 1> 0.022 71.3
KCl (mp-23193) <1 1 0> <1 1 0> 0.023 58.2
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.025 285.3
KCl (mp-23193) <1 0 0> <1 0 0> 0.028 41.2
C (mp-66) <1 1 1> <1 1 1> 0.033 285.3
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.037 174.7
Ge (mp-32) <1 0 0> <1 0 0> 0.039 164.7
C (mp-66) <1 0 0> <1 0 0> 0.042 164.7
ZnO (mp-2133) <0 0 1> <1 0 0> 0.046 329.4
MgO (mp-1265) <1 1 0> <1 1 0> 0.051 233.0
Al (mp-134) <1 0 0> <1 0 0> 0.056 82.4
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.058 174.7
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.060 247.1
MgO (mp-1265) <1 0 0> <1 0 0> 0.061 164.7
SiC (mp-8062) <1 0 0> <1 0 0> 0.063 329.4
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.066 71.3
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.067 174.7
GaN (mp-804) <0 0 1> <1 0 0> 0.078 288.3
Ni (mp-23) <1 1 0> <1 0 0> 0.081 329.4
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.087 233.0
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.088 285.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.090 82.4
Au (mp-81) <1 1 1> <1 1 1> 0.093 214.0
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.094 329.4
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.103 214.0
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.110 174.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.111 82.4
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.111 164.7
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.133 142.7
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.134 205.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.143 329.4
Ni (mp-23) <1 0 0> <1 0 0> 0.154 205.9
GaP (mp-2490) <1 1 1> <1 1 1> 0.156 214.0
Cu (mp-30) <1 0 0> <1 0 0> 0.158 205.9
NaCl (mp-22862) <1 0 0> <1 0 0> 0.166 164.7
GaP (mp-2490) <1 1 0> <1 1 0> 0.167 174.7
Ag (mp-124) <1 1 1> <1 1 1> 0.171 214.0
Mg (mp-153) <0 0 1> <1 1 0> 0.190 174.7
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.205 174.7
WS2 (mp-224) <0 0 1> <1 1 0> 0.205 174.7
CdS (mp-672) <1 1 1> <1 0 0> 0.208 205.9
TbScO3 (mp-31119) <0 1 0> <1 1 0> 0.234 174.7
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.237 329.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
113 3 3 0 0 0
3 113 3 0 0 0
3 3 113 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 17
Compliance Tensor Sij (10-12Pa-1)
8.9 -0.2 -0.2 0 0 0
-0.2 8.9 -0.2 0 0 0
-0.2 -0.2 8.9 0 0 0
0 0 0 60 0 0
0 0 0 0 60 0
0 0 0 0 0 60
Shear Modulus GV
32 GPa
Bulk Modulus KV
40 GPa
Shear Modulus GR
23 GPa
Bulk Modulus KR
40 GPa
Shear Modulus GVRH
28 GPa
Bulk Modulus KVRH
40 GPa
Elastic Anisotropy
1.93
Poisson's Ratio
0.22

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -3.862 32.939 2.265 6.206
pack_evans_james -3.862 32.941 0.251 3.406
vinet -3.862 32.921 2.305 5.198
tait -3.862 32.917 0.254 5.541
birch_euler -3.862 32.936 0.284 0.412
pourier_tarantola -3.863 32.916 0.044 2.442
birch_lagrange -3.868 32.942 0.162 6.061
murnaghan -3.861 32.972 0.245 3.282
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.114 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
TiC (mp-631) 0.0000 0.000 2
PuS (mp-2086) 0.0000 0.000 2
ErP (mp-1144) 0.0000 0.000 2
TmS (mp-1766) 0.0000 0.000 2
AgI (mp-22919) 0.0000 0.093 2
As (mp-10) 0.0000 0.112 1
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sn_d Te
Final Energy/Atom
-3.8626 eV
Corrected Energy
-8.1472 eV
Uncorrected energy = -7.7252 eV Composition-based energy adjustment (-0.422 eV/atom x 1.0 atoms) = -0.4220 eV Corrected energy = -8.1472 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 52489
  • 652760
  • 652744
  • 652756
  • 652761
  • 600865
  • 652763
  • 652745
  • 652742
  • 604177
  • 600813
  • 652741
  • 601065
  • 652750
  • 652755
  • 652753
  • 652751
  • 652749
  • 652752
  • 600136
  • 652754
  • 652746
  • 652759
Submitted by
User remarks:
  • Tin telluride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)