Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.959 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
13.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 57928 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.000 283.3
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.000 72.9
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.000 103.0
LiF (mp-1138) <1 1 0> <1 1 0> 0.002 141.7
KCl (mp-23193) <1 0 0> <1 0 0> 0.004 82.0
AlN (mp-661) <0 0 1> <1 1 1> 0.004 110.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.004 115.9
C (mp-48) <0 0 1> <1 1 1> 0.009 15.8
Al (mp-134) <1 0 0> <1 0 0> 0.026 82.0
MgO (mp-1265) <1 0 0> <1 0 0> 0.031 18.2
MgO (mp-1265) <1 1 0> <1 1 0> 0.032 25.8
Ge (mp-32) <1 1 0> <1 1 0> 0.034 141.7
CdWO4 (mp-19387) <1 1 0> <1 1 0> 0.037 244.7
TiO2 (mp-390) <0 0 1> <1 0 0> 0.038 72.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.038 163.9
GaN (mp-804) <0 0 1> <1 1 1> 0.043 63.1
Mg (mp-153) <1 1 0> <1 1 0> 0.050 115.9
GaN (mp-804) <1 1 0> <1 1 0> 0.065 115.9
GaAs (mp-2534) <1 0 0> <1 0 0> 0.083 163.9
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.088 82.0
Mg (mp-153) <1 0 0> <1 1 0> 0.101 115.9
MoS2 (mp-1434) <1 0 0> <1 1 0> 0.110 270.5
GaAs (mp-2534) <1 1 0> <1 1 0> 0.110 141.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.113 118.4
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.115 209.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.115 38.6
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.117 205.1
Si (mp-149) <1 0 0> <1 0 0> 0.124 118.4
Si (mp-149) <1 1 1> <1 1 1> 0.128 205.1
PbS (mp-21276) <1 0 0> <1 0 0> 0.128 36.4
PbS (mp-21276) <1 1 0> <1 1 0> 0.131 51.5
PbS (mp-21276) <1 1 1> <1 1 1> 0.132 63.1
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.132 191.2
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.134 244.7
LiAlO2 (mp-3427) <0 0 1> <1 1 0> 0.140 193.2
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.141 264.1
AlN (mp-661) <1 1 0> <1 1 1> 0.146 189.3
C (mp-48) <1 1 1> <1 0 0> 0.177 100.2
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.180 141.7
TiO2 (mp-390) <1 1 1> <1 1 0> 0.191 322.0
Ge (mp-32) <1 0 0> <1 0 0> 0.191 163.9
AlN (mp-661) <1 0 1> <1 1 0> 0.198 90.2
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.199 191.2
ZnO (mp-2133) <1 0 0> <1 1 1> 0.200 157.7
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.205 91.1
Ni (mp-23) <1 1 0> <1 1 0> 0.211 51.5
Ni (mp-23) <1 1 1> <1 1 1> 0.212 63.1
ZrO2 (mp-2858) <1 0 -1> <1 1 0> 0.220 180.3
SiO2 (mp-6930) <1 1 1> <1 1 1> 0.227 157.7
DyScO3 (mp-31120) <0 1 1> <1 0 0> 0.227 318.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
366 161 161 0 0 0
161 366 161 0 0 0
161 161 366 0 0 0
0 0 0 125 0 0
0 0 0 0 125 0
0 0 0 0 0 125
Compliance Tensor Sij (10-12Pa-1)
3.7 -1.1 -1.1 0 0 0
-1.1 3.7 -1.1 0 0 0
-1.1 -1.1 3.7 0 0 0
0 0 0 8 0 0
0 0 0 0 8 0
0 0 0 0 0 8
Shear Modulus GV
116 GPa
Bulk Modulus KV
229 GPa
Shear Modulus GR
115 GPa
Bulk Modulus KR
229 GPa
Shear Modulus GVRH
116 GPa
Bulk Modulus KVRH
229 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HoTmZn2 (mp-983126) 0.0000 0.000 3
Pm2PtAu (mp-982772) 0.0000 0.000 3
Nd2IrAu (mp-973606) 0.0000 0.057 3
YbPrPd2 (mp-981530) 0.0000 0.011 3
YTmAl2 (mp-980662) 0.0000 0.016 3
TiFeCoSb (mp-998973) 0.0000 0.186 4
TiAlFeCo (mp-998980) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.028 4
VFeCoSi (mp-1066609) 0.0000 0.002 4
VFeCoSb (mp-1066862) 0.0000 0.163 4
ErPd (mp-851) 0.0000 0.000 2
YbRu (mp-567116) 0.0000 0.294 2
PrIn (mp-20023) 0.0000 0.000 2
ReC (mp-1009731) 0.0000 1.115 2
ScCu (mp-1169) 0.0000 0.000 2
Cu (mp-998890) 0.0000 0.037 1
Kr (mp-974400) 0.0000 0.002 1
H2 (mp-632250) 0.0000 0.000 1
Ge (mp-998883) 0.0000 0.339 1
U (mp-108) 0.0000 0.269 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Ir
Final Energy/Atom
-7.2510 eV
Corrected Energy
-14.5020 eV
-14.5020 eV = -14.5020 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 608240
  • 608241
  • 57928
Submitted by
User remarks:
  • Aluminium iridium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)