material

MoO3

ID:

mp-18856

DOI:

10.17188/1193562


Tags: Molybdenum oxide Molybdenum trioxide - beta prime

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.925 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.12 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.649 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 202324 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <1 1 1> <1 0 0> 0.003 170.0
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.004 85.0
C (mp-48) <1 0 0> <0 0 1> 0.012 58.0
LiNbO3 (mp-3731) <1 0 1> <0 0 1> 0.012 231.9
BaTiO3 (mp-5986) <1 0 1> <1 0 -1> 0.012 187.3
NaCl (mp-22862) <1 0 0> <1 1 -1> 0.012 258.8
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.012 116.0
KTaO3 (mp-3614) <1 0 0> <1 1 -1> 0.014 258.8
SiC (mp-7631) <0 0 1> <1 0 -1> 0.015 124.9
SiC (mp-11714) <0 0 1> <1 0 -1> 0.016 124.9
Si (mp-149) <1 1 1> <1 0 -1> 0.017 312.2
CeO2 (mp-20194) <1 1 1> <1 0 -1> 0.018 312.2
Si (mp-149) <1 1 0> <1 0 0> 0.022 85.0
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.022 85.0
Al (mp-134) <1 0 0> <1 1 -1> 0.023 258.8
YAlO3 (mp-3792) <1 1 0> <0 1 1> 0.024 166.2
Mg (mp-153) <1 0 0> <1 0 -1> 0.029 249.7
YAlO3 (mp-3792) <1 0 0> <0 1 0> 0.029 119.1
GaP (mp-2490) <1 1 1> <1 0 -1> 0.030 312.2
Cu (mp-30) <1 0 0> <1 1 -1> 0.031 258.8
GdScO3 (mp-5690) <1 0 0> <1 0 -1> 0.031 187.3
GaP (mp-2490) <1 1 0> <1 0 0> 0.032 85.0
LiGaO2 (mp-5854) <1 1 0> <0 1 0> 0.032 238.2
CdS (mp-672) <1 1 1> <1 1 -1> 0.035 258.8
GaN (mp-804) <1 0 0> <1 0 -1> 0.036 249.7
MgO (mp-1265) <1 1 0> <0 0 1> 0.042 231.9
ZrO2 (mp-2858) <0 0 1> <1 0 -1> 0.043 249.7
Cu (mp-30) <1 1 1> <0 1 1> 0.043 249.3
ZrO2 (mp-2858) <0 1 0> <1 0 -1> 0.044 249.7
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.045 173.9
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.046 85.0
BN (mp-984) <1 1 0> <1 0 0> 0.047 170.0
SrTiO3 (mp-4651) <1 1 0> <1 0 -1> 0.047 62.4
CaF2 (mp-2741) <1 1 1> <1 0 -1> 0.048 312.2
GaN (mp-804) <0 0 1> <0 1 1> 0.048 249.3
YAlO3 (mp-3792) <0 0 1> <1 0 -1> 0.049 249.7
CdS (mp-672) <1 0 0> <1 0 -1> 0.056 312.2
GaN (mp-804) <1 1 0> <1 0 1> 0.057 262.9
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.058 170.0
CdS (mp-672) <1 0 1> <0 0 1> 0.059 231.9
Fe2O3 (mp-24972) <0 0 1> <0 1 1> 0.060 249.3
TiO2 (mp-390) <1 1 0> <1 0 -1> 0.061 312.2
SiC (mp-8062) <1 0 0> <1 0 -1> 0.065 249.7
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.067 255.1
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.069 231.9
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.069 178.7
TbScO3 (mp-31119) <1 0 0> <1 0 -1> 0.071 187.3
SrTiO3 (mp-4651) <0 0 1> <1 0 -1> 0.071 62.4
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.075 255.1
YAlO3 (mp-3792) <1 1 1> <0 1 1> 0.076 249.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
65 29 1 0 -2 0
29 73 -5 0 -4 0
1 -5 112 0 -2 0
0 0 0 55 0 2
-2 -4 -2 0 36 0
0 0 0 2 0 29
Compliance Tensor Sij (10-12Pa-1)
18.7 -7.4 -0.5 0 0.1 0
-7.4 16.8 0.9 0 1.6 0
-0.5 0.9 9 0 0.6 0
0 0 0 18.2 0 -1.2
0.1 1.6 0.6 0 28.2 0
0 0 0 -1.2 0 34.6
Shear Modulus GV
39 GPa
Bulk Modulus KV
33 GPa
Shear Modulus GR
33 GPa
Bulk Modulus KR
33 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
33 GPa
Elastic Anisotropy
0.85
Poisson's Ratio
0.10

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
V2(OF)3 (mp-778922) 0.4767 0.023 3
VO2F (mp-763096) 0.4348 0.018 3
V4O7F5 (mp-777229) 0.4518 0.020 3
V4O7F5 (mp-764881) 0.4138 0.018 3
V4O7F5 (mp-763970) 0.4486 0.018 3
NiC2(SN)2 (mp-8129) 0.7230 0.232 4
CdC2(SN)2 (mp-540903) 0.7026 0.184 4
MoO3 (mvc-14941) 0.4193 0.010 2
HgI2 (mp-23173) 0.7173 0.021 2
MoO3 (mp-715463) 0.6865 0.038 2
MoO3 (mp-715584) 0.3491 0.003 2
MoO3 (mp-510584) 0.7242 0.039 2
RbCdC3(SN)3 (mp-540654) 0.7329 0.111 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

A 16 wt-% MoO3/Al2O3 catalyst was prepared on a -Al2O3 support (Condea, Germany) [BET surface area: 280 m2g1, total pore volume: 0.7 mLg1, total acidity: 0.31 mmolg1 (strong)] by an incipient w [...]
MoO3/Al2O3 systems have been prepared by calcining at 770 K alumina impregnated with ammonium heptamolybdate (aq), or by calcining molybdena/alumina mixtures at 770 K. Surface polymolybdates have been [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition MoO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mo: 4.38 eV
Pseudopotentials
VASP PAW: Mo_pv O
Final Energy/Atom
-7.0312 eV
Corrected Energy
-267.1026 eV
Uncorrected energy = -224.9986 eV Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV Composition-based energy adjustment (-3.202 eV/atom x 8.0 atoms) = -25.6160 eV Corrected energy = -267.1026 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 644067
  • 202324
  • 644068
Submitted by
User remarks:
  • Molybdenum oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)