material

Sr3(FeO3)2

ID:

mp-18924

DOI:

10.17188/1193661


Tags: Tristrontium diiron(III) oxide

Material Details

Final Magnetic Moment
10.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.613 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.322 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 0 0> <0 0 1> 0.018 141.2
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.020 156.9
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.027 78.4
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.028 219.6
C (mp-48) <1 1 0> <0 0 1> 0.036 266.7
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.039 226.4
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.040 360.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.041 62.8
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.057 62.8
ZnO (mp-2133) <1 1 0> <0 0 1> 0.070 360.8
AlN (mp-661) <0 0 1> <1 1 1> 0.081 228.5
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.082 235.3
PbSe (mp-2201) <1 0 0> <0 0 1> 0.082 78.4
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.087 219.6
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.091 31.4
Au (mp-81) <1 1 1> <1 0 0> 0.107 240.1
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.118 62.8
GaN (mp-804) <0 0 1> <0 0 1> 0.121 172.6
GaSb (mp-1156) <1 0 0> <0 0 1> 0.122 78.4
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.122 313.8
Au (mp-81) <1 0 0> <0 0 1> 0.127 141.2
Au (mp-81) <1 1 0> <1 0 1> 0.131 244.7
Mg (mp-153) <1 0 0> <0 0 1> 0.144 235.3
BN (mp-984) <1 0 1> <0 0 1> 0.150 203.9
Mg (mp-153) <1 0 1> <0 0 1> 0.154 266.7
CsI (mp-614603) <1 0 0> <0 0 1> 0.157 62.8
CdSe (mp-2691) <1 0 0> <0 0 1> 0.159 78.4
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.164 113.2
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.193 251.0
ZnO (mp-2133) <1 0 0> <0 0 1> 0.196 172.6
C (mp-66) <1 0 0> <0 0 1> 0.209 62.8
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.211 226.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.214 282.4
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.216 47.1
GaP (mp-2490) <1 1 1> <0 0 1> 0.222 156.9
ZnO (mp-2133) <1 0 1> <0 0 1> 0.227 219.6
Ag (mp-124) <1 0 0> <0 0 1> 0.235 141.2
Ni (mp-23) <1 0 0> <0 0 1> 0.241 62.8
Si (mp-149) <1 1 1> <0 0 1> 0.248 156.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.253 156.9
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.254 298.1
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.254 156.9
GaSe (mp-1943) <0 0 1> <0 0 1> 0.256 298.1
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.266 244.7
ZnO (mp-2133) <1 1 1> <1 1 0> 0.268 226.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.271 282.4
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.279 15.7
PbS (mp-21276) <1 0 0> <0 0 1> 0.281 141.2
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.283 188.3
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.290 251.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
172 111 57 0 0 0
111 172 57 0 0 0
57 57 188 0 0 0
0 0 0 51 0 0
0 0 0 0 51 0
0 0 0 0 0 90
Compliance Tensor Sij (10-12Pa-1)
10.2 -6.2 -1.2 0 0 0
-6.2 10.2 -1.2 0 0 0
-1.2 -1.2 6.1 0 0 0
0 0 0 19.6 0 0
0 0 0 0 19.6 0
0 0 0 0 0 11.1
Shear Modulus GV
59 GPa
Bulk Modulus KV
109 GPa
Shear Modulus GR
52 GPa
Bulk Modulus KR
108 GPa
Shear Modulus GVRH
55 GPa
Bulk Modulus KVRH
109 GPa
Elastic Anisotropy
0.73
Poisson's Ratio
0.28

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.77 0.00 0.00
0.00 4.77 0.00
0.00 0.00 4.20
Dielectric Tensor εij (total)
25.05 0.00 0.00
0.00 25.05 0.00
0.00 0.00 13.29
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.58
Polycrystalline dielectric constant εpoly
(total)
21.13
Refractive Index n
2.14
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
La3(VN3)2 (mp-31054) 0.2738 0.000 3
Ba3In2O6 (mp-20352) 0.1398 0.000 3
La3(CrN3)2 (mp-569565) 0.2571 0.000 3
La3(TaN3)2 (mp-29964) 0.1564 0.000 3
La3(NbN3)2 (mp-10558) 0.1634 0.000 3
Sr2YCu2AgO7 (mvc-288) 0.7098 0.060 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
700 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Sr_sv Fe_pv O
Final Energy/Atom
-6.4328 eV
Corrected Energy
-79.3953 eV
Uncorrected energy = -70.7613 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Composition-based energy adjustment (-2.256 eV/atom x 2.0 atoms) = -4.5120 eV Corrected energy = -79.3953 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 249014
  • 74434
  • 249015
Submitted by
User remarks:
  • Tristrontium diiron(III) oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)