Material Details

Final Magnetic Moment
2.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.732 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.88 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.873 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [167]
Hall
-R 3 2"c
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 45060 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.000 76.1
CdTe (mp-406) <1 1 1> <0 0 1> 0.000 76.1
Au (mp-81) <1 1 1> <0 0 1> 0.000 361.4
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.001 57.1
InSb (mp-20012) <1 1 1> <0 0 1> 0.002 76.1
SiC (mp-8062) <1 1 1> <0 0 1> 0.003 133.2
GaAs (mp-2534) <1 1 1> <0 0 1> 0.009 57.1
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.012 361.4
Ag (mp-124) <1 1 1> <0 0 1> 0.015 361.4
Te2W (mp-22693) <0 1 0> <1 0 1> 0.021 216.2
GaN (mp-804) <0 0 1> <0 0 1> 0.025 171.2
InP (mp-20351) <1 1 1> <0 0 1> 0.026 247.3
GaAs (mp-2534) <1 0 0> <0 0 1> 0.032 361.4
LiF (mp-1138) <1 0 0> <0 0 1> 0.035 133.2
Ge (mp-32) <1 1 1> <0 0 1> 0.048 57.1
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.048 152.2
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.053 69.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.061 76.1
CdWO4 (mp-19387) <1 1 1> <1 0 0> 0.066 208.5
PbS (mp-21276) <1 1 1> <0 0 1> 0.070 247.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.072 190.2
BN (mp-984) <0 0 1> <0 0 1> 0.077 171.2
C (mp-48) <0 0 1> <0 0 1> 0.077 133.2
AlN (mp-661) <1 0 1> <0 0 1> 0.083 323.4
TePb (mp-19717) <1 0 0> <0 0 1> 0.084 304.4
BN (mp-984) <1 1 1> <1 1 0> 0.089 240.8
Ge (mp-32) <1 0 0> <0 0 1> 0.089 361.4
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.094 208.5
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.108 342.4
CdTe (mp-406) <1 0 0> <0 0 1> 0.120 304.4
TePb (mp-19717) <1 1 0> <0 0 1> 0.133 304.4
NaCl (mp-22862) <1 1 0> <0 0 1> 0.140 228.3
InSb (mp-20012) <1 0 0> <0 0 1> 0.141 304.4
Te2Mo (mp-602) <1 0 0> <1 0 1> 0.151 216.2
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.164 139.0
AlN (mp-661) <1 1 0> <1 1 0> 0.164 240.8
AlN (mp-661) <1 0 0> <1 0 0> 0.164 139.0
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.172 152.2
LiF (mp-1138) <1 1 0> <0 0 1> 0.175 95.1
CdS (mp-672) <1 0 1> <0 0 1> 0.178 228.3
GaN (mp-804) <1 0 0> <1 0 1> 0.197 216.2
Te2W (mp-22693) <0 0 1> <1 1 1> 0.209 243.8
NaCl (mp-22862) <1 1 1> <0 0 1> 0.210 57.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.214 57.1
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.221 304.4
SiC (mp-7631) <0 0 1> <0 0 1> 0.229 57.1
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.232 304.4
GaN (mp-804) <1 1 1> <1 0 0> 0.250 278.0
TePb (mp-19717) <1 1 1> <0 0 1> 0.257 76.1
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.260 266.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
360 149 111 19 0 0
149 360 111 -19 0 0
111 111 229 0 0 0
19 -19 0 80 0 0
0 0 0 0 80 19
0 0 0 0 19 106
Compliance Tensor Sij (10-12Pa-1)
3.7 -1.2 -1.2 -1.2 0 0
-1.2 3.7 -1.2 1.2 0 0
-1.2 -1.2 5.5 0 0 0
-1.2 1.2 0 13.1 0 0
0 0 0 0 13.1 -2.4
0 0 0 0 -2.4 9.9
Shear Modulus GV
92 GPa
Bulk Modulus KV
188 GPa
Shear Modulus GR
86 GPa
Bulk Modulus KR
176 GPa
Shear Modulus GVRH
89 GPa
Bulk Modulus KVRH
182 GPa
Elastic Anisotropy
0.40
Poisson's Ratio
0.29

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.74 -0.00 -0.00
-0.00 4.74 -0.00
-0.00 -0.00 4.31
Dielectric Tensor εij (total)
9.52 -0.00 -0.00
-0.00 9.52 -0.00
-0.00 -0.00 9.82
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.60
Polycrystalline dielectric constant εpoly
(total)
9.62
Refractive Index n
2.14
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiBO3 (mp-9716) 0.0118 0.073 3
MnBO3 (mp-761288) 0.0097 0.042 3
FeBO3 (mp-19097) 0.0151 0.000 3
CrBO3 (mp-19299) 0.0228 0.000 3
GaBO3 (mp-1078259) 0.0391 0.004 3
LiMn(CO3)2 (mp-769558) 0.2057 0.022 4
LiV(CO3)2 (mp-762019) 0.2143 0.000 4
LiFe(CO3)2 (mp-768029) 0.2112 0.000 4
MnSn(BO3)2 (mp-25012) 0.2018 0.000 4
SiH12C2(NF)6 (mp-697253) 0.7239 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: V_pv B O
Final Energy/Atom
-8.0959 eV
Corrected Energy
-88.5365 eV
-88.5365 eV = -80.9588 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 45060
  • 419132
Submitted by
User remarks:
  • Vanadium(III) borate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)