Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.531 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Group3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 133.8 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 189.3 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 283.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 200.7 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 283.9 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 133.8 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 94.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 66.9 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 283.9 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 267.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 267.6 |
InP (mp-20351) | <1 0 0> | <1 1 0> | 283.9 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 200.7 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 133.8 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 94.6 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 66.9 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 189.3 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 189.3 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 267.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 94.6 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 267.6 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 283.9 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 283.9 |
Si (mp-149) | <1 0 0> | <1 0 0> | 267.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 200.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 267.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 66.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 94.6 |
C (mp-48) | <1 0 1> | <1 0 0> | 200.7 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 115.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 267.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 283.9 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 115.9 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 66.9 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 94.6 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 133.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 133.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 94.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 189.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 66.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 94.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 283.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 267.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 66.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 94.6 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 115.9 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 267.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 267.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 189.3 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 133.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaBiO3 (mp-545783) | 0.1233 | 0.021 | 3 |
Fe(NF2)3 (mp-1079464) | 0.1214 | 1.402 | 3 |
Ti(NF2)3 (mp-1080110) | 0.1117 | 1.493 | 3 |
Co(IN2)3 (mp-1078734) | 0.1370 | 2.051 | 3 |
Co(IN2)3 (mp-1084766) | 0.1120 | 2.051 | 3 |
Ca6In2NF (mp-989404) | 0.0030 | 0.000 | 4 |
Ca6Al2NF (mp-989399) | 0.0160 | 0.014 | 4 |
Sr2ZnMoO6 (mp-18829) | 0.0224 | 0.025 | 4 |
Ba2NiMoO6 (mp-561738) | 0.0154 | 0.000 | 4 |
Ba2ReNiO6 (mp-32306) | 0.0201 | 0.052 | 4 |
Ca3Sb2 (mp-1013546) | 0.2258 | 0.421 | 2 |
Ba3Sb2 (mp-1013582) | 0.2258 | 0.416 | 2 |
Fe4N (mp-535) | 0.2258 | 0.070 | 2 |
Ca3Bi2 (mp-1013735) | 0.2258 | 0.363 | 2 |
Sr3Sb2 (mp-1013583) | 0.2258 | 0.378 | 2 |
BaLiPrTeO6 (mp-41219) | 0.1108 | 0.070 | 5 |
BaLaTaMnO6 (mp-41283) | 0.1134 | 0.117 | 5 |
BaLiLaTeO6 (mp-40189) | 0.1098 | 0.030 | 5 |
BaLaMnMoO6 (mp-40356) | 0.1172 | 0.189 | 5 |
BaLaTaMnO6 (mp-622599) | 0.1137 | 0.117 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7287 | 0.065 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVMo: 4.38 eV |
PseudopotentialsVASP PAW: Ba_sv Co Mo_pv O |
Final Energy/Atom-6.7176 eV |
Corrected Energy-153.5888 eV
-153.5888 eV = -134.3513 eV (uncorrected energy) - 10.8100 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)