material

FeCO3

ID:

mp-18969

DOI:

10.17188/1193744


Tags: Siderite Iron carbonate High pressure experimental phase

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.790 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.78 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [167]
Hall
-R 3 2"c
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 100678 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 1 0> <0 0 1> -0.363 138.3
LiGaO2 (mp-5854) <1 1 1> <0 0 1> -0.362 335.9
Al (mp-134) <1 1 0> <0 0 1> -0.359 138.3
BN (mp-984) <1 1 1> <0 0 1> -0.283 237.1
InP (mp-20351) <1 0 0> <0 0 1> -0.223 177.8
ZnSe (mp-1190) <1 0 0> <0 0 1> -0.223 98.8
GaAs (mp-2534) <1 0 0> <0 0 1> -0.211 98.8
Al (mp-134) <1 0 0> <0 0 1> -0.201 98.8
Ge (mp-32) <1 0 0> <0 0 1> -0.175 98.8
KTaO3 (mp-3614) <1 0 0> <0 0 1> -0.163 98.8
PbS (mp-21276) <1 0 0> <0 0 1> -0.157 177.8
NaCl (mp-22862) <1 0 0> <0 0 1> -0.124 98.8
LiF (mp-1138) <1 0 0> <0 0 1> -0.122 98.8
GdScO3 (mp-5690) <0 1 0> <0 0 1> -0.113 316.1
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> -0.107 197.6
Cu (mp-30) <1 1 0> <0 0 1> -0.064 296.4
GdScO3 (mp-5690) <1 0 0> <0 0 1> -0.063 237.1
LiGaO2 (mp-5854) <1 0 0> <0 0 1> -0.062 316.1
ZrO2 (mp-2858) <0 1 0> <0 0 1> -0.055 335.9
Au (mp-81) <1 1 0> <0 0 1> -0.055 98.8
C (mp-48) <1 1 1> <0 0 1> -0.027 237.1
Ge (mp-32) <1 1 0> <0 0 1> -0.027 237.1
TeO2 (mp-2125) <0 0 1> <0 0 1> -0.026 355.7
LaF3 (mp-905) <1 1 0> <0 0 1> -0.020 276.6
Ag (mp-124) <1 1 0> <0 0 1> -0.019 98.8
Ag (mp-124) <1 0 0> <0 0 1> -0.016 138.3
ZrO2 (mp-2858) <1 0 0> <0 0 1> -0.005 316.1
ZnO (mp-2133) <0 0 1> <0 0 1> 0.001 177.8
AlN (mp-661) <0 0 1> <0 0 1> 0.001 59.3
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.001 316.1
Au (mp-81) <1 0 0> <0 0 1> 0.002 138.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.008 79.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.008 79.0
Ni (mp-23) <1 1 1> <0 0 1> 0.009 256.9
WSe2 (mp-1821) <1 0 1> <1 1 0> 0.014 253.4
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.016 158.1
Te2W (mp-22693) <1 0 0> <1 0 0> 0.019 292.6
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.019 219.5
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.021 296.4
GaAs (mp-2534) <1 1 0> <0 0 1> 0.021 237.1
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.021 316.1
TiO2 (mp-390) <0 0 1> <1 0 1> 0.023 303.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.034 253.4
AlN (mp-661) <1 0 0> <0 0 1> 0.041 375.4
YVO4 (mp-19133) <1 1 1> <1 1 0> 0.045 253.4
Al (mp-134) <1 1 1> <0 0 1> 0.050 256.9
GaTe (mp-542812) <1 0 0> <0 0 1> 0.054 177.8
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.060 237.1
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.062 253.4
GaSe (mp-1943) <0 0 1> <0 0 1> 0.066 237.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
157 162 72 17 0 0
162 157 72 -17 0 0
72 72 126 0 0 0
17 -17 0 37 0 0
0 0 0 0 37 17
0 0 0 0 17 -2
Compliance Tensor Sij (10-12Pa-1)
-22.3 26.5 -2.4 22.9 0 0
26.5 -22.3 -2.4 -22.9 0 0
-2.4 -2.4 10.7 0 0 0
22.9 -22.9 0 5.8 0 0
0 0 0 0 5.8 45.7
0 0 0 0 45.7 -97.6
Shear Modulus GV
23 GPa
Bulk Modulus KV
117 GPa
Shear Modulus GR
-31 GPa
Bulk Modulus KR
105 GPa
Shear Modulus GVRH
-4 GPa
Bulk Modulus KVRH
111 GPa
Elastic Anisotropy
-8.63
Poisson's Ratio
0.52

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCO3 (mp-9812) 0.1088 0.000 3
FeCO3 (mp-909679) 0.1071 0.000 3
CoCO3 (mp-24854) 0.0284 0.000 3
MnCO3 (mp-18814) 0.1104 0.000 3
MnCO3 (mp-818781) 0.1099 0.000 3
LiMn(CO3)2 (mp-769558) 0.1927 0.022 4
LiV(CO3)2 (mp-762019) 0.2312 0.000 4
LiFe(CO3)2 (mp-768029) 0.2370 0.000 4
MgSn(BO3)2 (mp-11715) 0.2048 0.000 4
MnSn(BO3)2 (mp-25012) 0.2330 0.000 4
SiH12C2(NF)6 (mp-697253) 0.7090 0.000 5
TiH12C2(NF)6 (mp-696940) 0.7414 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv C O
Final Energy/Atom
-7.4349 eV
Corrected Energy
-82.9832 eV
Uncorrected energy = -74.3492 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Composition-based energy adjustment (-2.256 eV/atom x 2.0 atoms) = -4.5120 eV Corrected energy = -82.9832 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 169798
  • 169795
  • 100678
  • 169789
  • 169796
  • 169793
  • 169797
  • 169792
  • 182821
  • 169791
  • 169794
  • 169790
Submitted by
User remarks:
  • Siderite
  • Iron carbonate
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)