material

BaCoO2

ID:

mp-19086

DOI:

10.17188/1193871


Tags: Barium cobalt oxide

Material Details

Final Magnetic Moment
3.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.052 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoO + BaO
Band Gap
0.526 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3121 [152]
Hall
P 31 2"
Point Group
32
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 25813 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 1 1> <1 0 1> 0.010 254.7
Ni (mp-23) <1 1 1> <1 0 1> 0.018 254.7
KTaO3 (mp-3614) <1 1 1> <1 0 1> 0.024 254.7
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.033 121.7
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 1 0> 0.041 210.8
C (mp-48) <0 0 1> <1 0 0> 0.047 162.3
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.050 277.2
SiC (mp-11714) <0 0 1> <1 0 1> 0.050 254.7
AlN (mp-661) <0 0 1> <1 0 0> 0.051 162.3
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.052 92.4
PbS (mp-21276) <1 1 0> <1 1 1> 0.054 153.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.055 277.2
SiC (mp-7631) <0 0 1> <1 0 1> 0.056 254.7
BN (mp-984) <0 0 1> <0 0 1> 0.059 215.6
ZnO (mp-2133) <0 0 1> <0 0 1> 0.061 123.2
MgO (mp-1265) <1 1 0> <1 0 0> 0.064 202.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.066 123.2
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.067 123.2
BaTiO3 (mp-5986) <0 0 1> <1 1 1> 0.068 306.9
GaN (mp-804) <1 0 0> <1 0 0> 0.073 284.0
GaSe (mp-1943) <0 0 1> <1 0 0> 0.081 162.3
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.090 284.0
KCl (mp-23193) <1 1 1> <0 0 1> 0.097 215.6
TiO2 (mp-390) <1 1 1> <0 0 1> 0.098 215.6
AlN (mp-661) <1 0 0> <1 0 1> 0.100 254.7
Ga2O3 (mp-886) <0 1 0> <0 0 1> 0.101 215.6
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.102 324.6
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.106 202.9
GaN (mp-804) <0 0 1> <1 0 1> 0.121 254.7
YAlO3 (mp-3792) <0 1 0> <1 1 1> 0.128 76.7
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.130 215.6
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.134 277.2
Mg (mp-153) <1 1 0> <1 1 1> 0.138 230.2
GaN (mp-804) <1 1 0> <1 1 1> 0.139 230.2
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.142 92.4
CdWO4 (mp-19387) <0 1 0> <0 0 1> 0.155 338.7
Mg (mp-153) <0 0 1> <0 0 1> 0.158 215.6
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.159 305.6
AlN (mp-661) <1 1 1> <1 0 0> 0.162 202.9
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.166 324.6
SiC (mp-11714) <1 0 0> <1 0 1> 0.175 254.7
MgO (mp-1265) <1 1 1> <0 0 1> 0.175 30.8
Cu (mp-30) <1 1 1> <0 0 1> 0.179 92.4
Ag (mp-124) <1 1 0> <1 0 0> 0.189 121.7
PbS (mp-21276) <1 1 1> <1 0 1> 0.199 254.7
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.202 162.3
TiO2 (mp-390) <1 0 1> <1 1 0> 0.211 281.1
SiC (mp-11714) <1 0 1> <1 0 1> 0.217 254.7
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.220 306.9
LiF (mp-1138) <1 1 1> <1 0 1> 0.220 254.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
117 61 59 3 0 0
61 117 59 -3 0 0
59 59 117 0 0 0
3 -3 0 34 0 0
0 0 0 0 34 3
0 0 0 0 3 28
Compliance Tensor Sij (10-12Pa-1)
13.2 -4.8 -4.2 -1.5 0 0
-4.8 13.2 -4.2 1.5 0 0
-4.2 -4.2 12.7 0 0 0
-1.5 1.5 0 29.5 0 0
0 0 0 0 29.5 -3
0 0 0 0 -3 36.1
Shear Modulus GV
31 GPa
Bulk Modulus KV
79 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
79 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
79 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.33

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
-1.05962 1.05928 0.00000 0.13464 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -0.13462 1.05928
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
1.50433 C/m2
Crystallographic Direction vmax
-1.00000
-0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.58 -0.00 -0.00
-0.00 4.58 0.00
-0.00 0.00 4.85
Dielectric Tensor εij (total)
14.80 -0.00 -0.00
-0.00 14.80 0.00
-0.00 0.00 17.78
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.67
Polycrystalline dielectric constant εpoly
(total)
15.79
Refractive Index n
2.16
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KCoO2 (mp-18895) 0.5849 0.083 3
BaMgO2 (mp-756018) 0.1581 0.038 3
CaSiN2 (mp-568965) 0.6067 0.000 3
BaZnO2 (mp-4236) 0.0595 0.000 3
KCoO2 (mp-640069) 0.5989 0.083 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
700 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Ba_sv Co O
Final Energy/Atom
-6.0293 eV
Corrected Energy
-81.3881 eV
Uncorrected energy = -72.3521 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Composition-based energy adjustment (-1.638 eV/atom x 3.0 atoms) = -4.9140 eV Corrected energy = -81.3881 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 25813
Submitted by
User remarks:
  • Barium cobalt oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)