Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.591 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.075 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCrP2O7 |
Band Gap3.190 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 200.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 229.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 119.5 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 205.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 199.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 199.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 292.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 258.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 199.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 355.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 229.2 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 256.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 291.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 226.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 199.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 355.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 258.7 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 291.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 226.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 263.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 85.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 199.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 158.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 229.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 205.3 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 267.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 229.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 199.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 199.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 226.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 119.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 57.3 |
CdS (mp-672) | <1 1 1> | <1 1 -1> | 200.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 199.2 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 238.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 229.2 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 292.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 318.7 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 226.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 258.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 226.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 329.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 234.1 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 229.2 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 291.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 175.6 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 329.0 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 226.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 258.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 171.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.04309 | 0.00000 | -0.17384 |
-0.31677 | -0.21443 | -0.21726 | 0.00000 | -0.01376 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.10944 | 0.00000 | 0.08223 |
Piezoelectric Modulus ‖eij‖max0.44013 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-2.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.97 | 0.00 | 0.08 |
0.00 | 3.06 | 0.00 |
0.08 | 0.00 | 3.16 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.72 | 0.00 | -0.08 |
0.00 | 6.22 | 0.00 |
-0.08 | 0.00 | 6.82 |
Polycrystalline dielectric constant
εpoly∞
3.07
|
Polycrystalline dielectric constant
εpoly
6.59
|
Refractive Index n1.75 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4017 | 0.020 | 3 |
Ni4P4O15 (mp-585202) | 0.4345 | 0.059 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3446 | 0.098 | 3 |
Ni4P4O15 (mp-705427) | 0.4325 | 0.059 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4156 | 0.366 | 3 |
LiVP2O7 (mp-18911) | 0.1215 | 0.025 | 4 |
LiMoP2O7 (mp-18987) | 0.2251 | 0.052 | 4 |
LiFeP2O7 (mp-19294) | 0.0984 | 0.166 | 4 |
LiScP2O7 (mp-10517) | 0.1835 | 0.000 | 4 |
LiTiP2O7 (mp-26629) | 0.2309 | 0.055 | 4 |
FeO2 (mvc-11999) | 0.7043 | 0.720 | 2 |
CrO2 (mvc-11581) | 0.7218 | 0.166 | 2 |
VO2 (mvc-6918) | 0.7466 | 0.095 | 2 |
Li2VCr(P2O7)2 (mp-763864) | 0.0831 | 0.012 | 5 |
Li2VCr(P2O7)2 (mp-764248) | 0.0776 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-764239) | 0.0742 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-763868) | 0.0854 | 0.012 | 5 |
Li2VCr(P2O7)2 (mp-763855) | 0.0853 | 0.000 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5631 | 0.257 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5280 | 0.331 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.7246 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5611 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-7.1448 eV |
Corrected Energy-171.0437 eV
-171.0437 eV = -157.1856 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)