Final Magnetic Moment4.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.333 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 50.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 146.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 207.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 41.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 264.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 164.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 329.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 234.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 164.8 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 164.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 123.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 88.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 264.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 264.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 146.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 123.6 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 252.8 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 50.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 176.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 82.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 202.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 164.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 329.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 247.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 206.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 88.0 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 288.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 146.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 247.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 202.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 164.8 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 50.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 247.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 29.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 291.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 291.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 82.4 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 130.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 202.3 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 151.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 146.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 264.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 151.7 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 164.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 234.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 146.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 205.3 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 254.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaGeO3 (mp-8130) | 0.0342 | 0.107 | 3 |
GdAlO3 (mp-5223) | 0.0786 | 0.012 | 3 |
CaTiO3 (mp-4019) | 0.0806 | 0.000 | 3 |
CaFeO3 (mvc-776) | 0.0215 | 0.000 | 3 |
CaMnO3 (mvc-11562) | 0.1011 | 0.035 | 3 |
Sr2UZnO6 (mp-554059) | 0.1146 | 0.054 | 4 |
CaPrTi2O6 (mvc-9241) | 0.1712 | 0.000 | 4 |
CaPrCr2O6 (mvc-9616) | 0.1541 | 0.042 | 4 |
CaPr(FeO3)2 (mvc-9650) | 0.1443 | 0.000 | 4 |
CaLaCr2O6 (mvc-9971) | 0.1646 | 0.029 | 4 |
Pb3O4 (mp-636813) | 0.7361 | 0.038 | 2 |
SrLaNiRuO6 (mp-694873) | 0.1778 | 0.000 | 5 |
Ca6Pr6Mn11CrO36 (mp-706248) | 0.1769 | 0.004 | 5 |
CaLaTiCrO6 (mvc-16468) | 0.1656 | 0.000 | 5 |
CaLaCrCoO6 (mvc-9966) | 0.1587 | 0.119 | 5 |
CaLaTiCrO6 (mp-39159) | 0.1833 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Ca_sv Fe_pv O |
Final Energy/Atom-6.4290 eV |
Corrected Energy-147.9399 eV
-147.9399 eV = -128.5804 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)