material

BaMnO3

ID:

mp-19156

DOI:

10.17188/1193980


Tags: Barium manganate(IV) Barium manganate(IV) - LT Barium manganate(IV) - alpha Barium manganate(IV) - 2H

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-2.494 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
< 0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.55 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
BaMnO3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 10331 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaN (mp-804) <1 0 1> <1 0 1> 0.002 286.8
BN (mp-984) <1 1 0> <1 0 0> 0.005 202.1
SrTiO3 (mp-4651) <1 1 0> <1 1 0> 0.009 250.1
GaAs (mp-2534) <1 1 1> <1 0 1> 0.009 286.8
AlN (mp-661) <0 0 1> <0 0 1> 0.010 261.5
ZnSe (mp-1190) <1 1 1> <1 0 1> 0.013 286.8
Ge (mp-32) <1 1 1> <1 0 1> 0.015 286.8
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.016 261.5
LiF (mp-1138) <1 1 1> <0 0 1> 0.016 29.1
MgAl2O4 (mp-3536) <1 1 1> <1 0 0> 0.018 115.5
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.023 231.0
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.024 115.5
CdS (mp-672) <1 1 0> <1 0 0> 0.026 346.5
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.032 203.4
WS2 (mp-224) <0 0 1> <1 0 0> 0.032 115.5
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.033 115.5
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.034 87.2
SrTiO3 (mp-4651) <0 0 1> <1 1 0> 0.036 250.1
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.038 231.0
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.039 200.1
PbSe (mp-2201) <1 1 1> <0 0 1> 0.040 203.4
YAlO3 (mp-3792) <1 0 0> <1 0 0> 0.044 202.1
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.044 231.0
GaTe (mp-542812) <1 0 0> <1 0 0> 0.046 317.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.047 29.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.047 29.1
ZnO (mp-2133) <1 0 0> <1 0 1> 0.050 122.9
C (mp-48) <0 0 1> <0 0 1> 0.052 203.4
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.057 86.6
GaN (mp-804) <0 0 1> <1 0 0> 0.063 115.5
GaSb (mp-1156) <1 1 1> <0 0 1> 0.063 203.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.066 202.1
Mg (mp-153) <0 0 1> <1 0 0> 0.067 115.5
CsI (mp-614603) <1 0 0> <1 1 0> 0.067 250.1
Ni (mp-23) <1 1 0> <1 0 0> 0.074 86.6
DyScO3 (mp-31120) <1 1 0> <1 1 0> 0.075 250.1
WSe2 (mp-1821) <1 1 0> <1 0 0> 0.075 86.6
ZrO2 (mp-2858) <1 1 1> <1 0 1> 0.076 204.8
BN (mp-984) <0 0 1> <1 0 0> 0.077 86.6
GaSe (mp-1943) <0 0 1> <0 0 1> 0.081 87.2
BaF2 (mp-1029) <1 0 0> <1 1 0> 0.082 200.1
CdSe (mp-2691) <1 1 1> <0 0 1> 0.086 203.4
TiO2 (mp-390) <0 0 1> <1 0 1> 0.096 286.8
SiC (mp-11714) <1 0 0> <1 1 0> 0.100 250.1
TiO2 (mp-390) <1 0 1> <1 0 0> 0.110 317.6
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.113 204.8
Ni (mp-23) <1 0 0> <1 1 0> 0.113 50.0
ZnSe (mp-1190) <1 0 0> <1 0 1> 0.113 163.9
Ni (mp-23) <1 1 1> <1 0 0> 0.113 86.6
TeO2 (mp-2125) <0 0 1> <1 0 1> 0.116 163.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
142 54 22 0 0 0
54 142 22 0 0 0
22 22 251 0 0 0
0 0 0 -2 0 0
0 0 0 0 -2 0
0 0 0 0 0 44
Compliance Tensor Sij (10-12Pa-1)
8.3 -3.1 -0.4 0 0 0
-3.1 8.3 -0.4 0 0 0
-0.4 -0.4 4.1 0 0 0
0 0 0 -525 0 0
0 0 0 0 -525 0
0 0 0 0 0 22.7
Shear Modulus GV
37 GPa
Bulk Modulus KV
81 GPa
Shear Modulus GR
-5 GPa
Bulk Modulus KR
79 GPa
Shear Modulus GVRH
16 GPa
Bulk Modulus KVRH
80 GPa
Elastic Anisotropy
-42.03
Poisson's Ratio
0.41

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba3NaN (mp-8868) 0.1580 0.000 3
BaCoO3 (mp-554938) 0.1598 0.002 3
CsNiF3 (mp-557772) 0.1608 0.000 3
BaNiO3 (mp-19138) 0.0748 0.000 3
Ba3LiN (mp-13288) 0.1267 0.028 3
Cs2LiGaF6 (mp-6654) 0.3365 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mn: 3.9 eV
Pseudopotentials
VASP PAW: Ba_sv Mn_pv O
Final Energy/Atom
-6.9213 eV
Corrected Energy
-153.5778 eV
-153.5778 eV = -138.4269 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 10332
  • 10331
  • 23873
  • 24129
  • 89994
Submitted by
User remarks:
  • Barium manganate(IV)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)