Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.866 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.022 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 214.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 155.1 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 130.9 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 267.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 155.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 155.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 155.1 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 303.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 218.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 217.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 138.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.0 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 43.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 279.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 155.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 341.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 87.2 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 214.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 174.5 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 53.5 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 247.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 341.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 217.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 248.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 155.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 53.5 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 174.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 31.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 43.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 43.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 53.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 61.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 131.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 93.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 155.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 160.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 155.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 217.1 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 107.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 227.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 218.1 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 261.7 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 261.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 155.1 |
YVO4 (mp-19133) | <0 0 1> | <1 1 -1> | 247.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 174.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 276.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 138.2 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 214.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 248.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmAlO3 (mp-7405) | 0.2081 | 0.000 | 3 |
LaGaO3 (mp-5837) | 0.1840 | 0.032 | 3 |
ZrPbO3 (mp-755798) | 0.2166 | 0.035 | 3 |
PrNiO3 (mp-25590) | 0.1398 | 0.000 | 3 |
BaCeO3 (mp-3187) | 0.2076 | 0.000 | 3 |
Sr2MgUO6 (mp-972112) | 0.1382 | 0.020 | 4 |
Sr2NbInO6 (mp-20222) | 0.1802 | 0.000 | 4 |
Sr2InSbO6 (mp-22355) | 0.1837 | 0.000 | 4 |
Sr2UCoO6 (mp-24886) | 0.1600 | 0.027 | 4 |
La2MnCoO6 (mp-556835) | 0.1530 | 0.000 | 4 |
FeSb3 (mp-971669) | 0.6856 | 0.000 | 2 |
Pb3O4 (mp-636813) | 0.6991 | 0.037 | 2 |
CoSb3 (mp-1317) | 0.7147 | 0.000 | 2 |
IrO3 (mp-1097041) | 0.7416 | 0.000 | 2 |
Pb2O3 (mp-690722) | 0.7448 | 0.212 | 2 |
CaLaTiFeO6 (mvc-8937) | 0.1780 | 0.000 | 5 |
CaLaCrFeO6 (mvc-8975) | 0.1273 | 0.017 | 5 |
CaLaVFeO6 (mvc-8988) | 0.1637 | 0.000 | 5 |
CaLaMnFeO6 (mvc-16539) | 0.1510 | 0.000 | 5 |
CaLaMnFeO6 (mp-40066) | 0.1619 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: La Mn_pv Co O |
Final Energy/Atom-7.6665 eV |
Corrected Energy-168.8665 eV
-168.8665 eV = -153.3293 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 7.1097 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)