Final Magnetic Moment0.187 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.990 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI43d [220] |
HallI 4bd 2c 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 253.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 119.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 253.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 253.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 169.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 84.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 119.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 169.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 84.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 84.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 119.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 253.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 253.8 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 84.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 119.6 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 239.3 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 253.8 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 253.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 253.8 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 84.6 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 119.6 |
Si (mp-149) | <1 1 1> | <1 0 0> | 253.8 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 253.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 119.6 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 239.3 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 239.3 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 169.2 |
MgF2 (mp-1249) | <1 1 1> | <1 1 0> | 119.6 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 169.2 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 169.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm(GdS2)2 (mp-676424) | 0.0653 | 0.027 | 3 |
Nd(SmSb)3 (mp-675554) | 0.0737 | 0.039 | 3 |
Ca(Nd2Se3)4 (mp-38586) | 0.0932 | 0.014 | 3 |
Tb2SmS4 (mp-38931) | 0.0886 | 0.062 | 3 |
YbPr11Se16 (mp-531712) | 0.0957 | 0.016 | 3 |
Gd3S4 (mp-20036) | 0.0083 | 0.013 | 2 |
Sm4Bi3 (mp-23283) | 0.0083 | 0.000 | 2 |
Y4Sb3 (mp-568320) | 0.0090 | 0.000 | 2 |
Tb4Sb3 (mp-2045) | 0.0131 | 0.015 | 2 |
Gd4Sb3 (mp-20831) | 0.0077 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Sb |
Final Energy/Atom-5.3918 eV |
Corrected Energy-75.4848 eV
-75.4848 eV = -75.4848 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)