material

CoO

ID:

mp-19275

DOI:

10.17188/1194158


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.278 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.132 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.24 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoO
Band Gap
1.261 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
mmm
Crystal System
tetragonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 199.8
LaAlO3 (mp-2920) <1 1 0> <1 1 1> 121.2
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 221.1
AlN (mp-661) <1 0 0> <1 0 1> 15.8
AlN (mp-661) <1 1 0> <1 0 1> 110.5
AlN (mp-661) <1 1 1> <1 0 1> 189.5
CeO2 (mp-20194) <1 1 0> <1 1 0> 160.4
AlN (mp-661) <0 0 1> <0 0 1> 66.6
AlN (mp-661) <1 0 1> <0 0 1> 104.7
GaAs (mp-2534) <1 1 1> <1 0 0> 176.5
CeO2 (mp-20194) <1 0 0> <0 0 1> 123.7
CeO2 (mp-20194) <1 1 1> <0 0 1> 256.9
BaF2 (mp-1029) <1 1 0> <1 1 1> 161.6
GaAs (mp-2534) <1 0 0> <1 0 0> 100.8
GaAs (mp-2534) <1 1 0> <1 1 0> 142.6
GaN (mp-804) <1 0 0> <1 0 0> 138.6
GaN (mp-804) <1 0 1> <1 0 1> 110.5
GaN (mp-804) <1 1 0> <1 0 0> 138.6
BaF2 (mp-1029) <1 0 0> <0 0 1> 38.1
GaN (mp-804) <0 0 1> <0 0 1> 190.3
GaN (mp-804) <1 1 1> <0 0 1> 123.7
SiO2 (mp-6930) <0 0 1> <1 1 0> 106.9
SiO2 (mp-6930) <1 0 0> <1 0 1> 110.5
SiO2 (mp-6930) <1 0 1> <1 0 1> 142.1
SiO2 (mp-6930) <1 1 0> <1 1 0> 142.6
KCl (mp-23193) <1 0 0> <0 0 1> 85.6
KCl (mp-23193) <1 1 0> <1 0 1> 236.9
KCl (mp-23193) <1 1 1> <1 0 1> 142.1
SiO2 (mp-6930) <1 1 1> <1 1 1> 161.6
DyScO3 (mp-31120) <0 0 1> <1 1 1> 282.9
DyScO3 (mp-31120) <1 0 0> <1 1 0> 142.6
DyScO3 (mp-31120) <1 0 1> <0 0 1> 333.0
DyScO3 (mp-31120) <1 1 0> <0 0 1> 123.7
DyScO3 (mp-31120) <0 1 0> <0 0 1> 180.8
DyScO3 (mp-31120) <0 1 1> <1 0 0> 315.1
InAs (mp-20305) <1 0 0> <0 0 1> 38.1
InAs (mp-20305) <1 1 0> <1 0 1> 157.9
InAs (mp-20305) <1 1 1> <1 1 0> 320.8
ZnSe (mp-1190) <1 0 0> <1 0 0> 100.8
ZnSe (mp-1190) <1 1 0> <1 1 0> 142.6
ZnSe (mp-1190) <1 1 1> <1 0 0> 176.5
KTaO3 (mp-3614) <1 0 0> <1 0 0> 50.4
KTaO3 (mp-3614) <1 1 0> <1 1 0> 71.3
KTaO3 (mp-3614) <1 1 1> <1 0 0> 201.7
CdS (mp-672) <1 0 1> <1 0 0> 63.0
CdS (mp-672) <1 1 0> <0 0 1> 294.9
CdS (mp-672) <0 0 1> <1 0 0> 88.2
CdS (mp-672) <1 0 0> <1 0 1> 110.5
CdS (mp-672) <1 1 1> <1 0 0> 163.8
LiF (mp-1138) <1 1 0> <1 1 0> 71.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
In4SbTe3 (mp-685941) 0.1732 0.022 3
GaCuTe2 (mp-676248) 0.1720 0.204 3
TiNbN2 (mp-35869) 0.1740 0.094 3
Mg10FeO11 (mp-761768) 0.1758 0.002 3
LiFe3O4 (mp-1097797) 0.1572 0.086 3
Li3Ti4VO8 (mp-764914) 0.1997 0.080 4
LiNi5O5F (mp-765891) 0.2001 0.060 4
Li2NiOF2 (mp-765789) 0.2163 0.038 4
LiNi2O2F (mp-765536) 0.1953 0.052 4
LiNi3O3F (mp-765309) 0.2039 0.070 4
CoO (mp-19079) 0.1707 0.037 2
HgO (mp-545619) 0.1884 0.148 2
FeO (mp-715262) 0.1646 0.009 2
KN (mp-1064647) 0.1736 1.464 2
CsI (mp-1078801) 0.1697 0.003 2
Hg (mp-982872) 0.2477 0.020 1
Se (mp-7755) 0.2646 0.181 1
K (mp-998881) 0.2695 0.120 1
Te (mp-10654) 0.1879 0.047 1
Te (mp-105) 0.2814 0.047 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The N-doped CoO (N-CoO) films were prepared by electrolysis of an N2-saturated 0.05M solution of CoCl2 in acetonitrile at 1.0V (vs. Ag/AgCl), which produced a black film on the cathodic ITO surface [...]
CoOMoO3/MgO and NiOMoO3/MgO catalysts were prepared from MoO3/MgO by impregnation with methanol solutions of Co nitrate and Ni nitrate, respectively, followed by calcination at 350C. The texture of [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition CoO.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Co: 3.32 eV
Pseudopotentials
VASP PAW: Co O
Final Energy/Atom
-6.0184 eV
Corrected Energy
-58.4522 eV
-58.4522 eV = -48.1471 eV (uncorrected energy) - 7.4960 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)