Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.579 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.789 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 0 0> | <0 0 1> | 202.0 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 228.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 202.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 231.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 173.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 228.6 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 261.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 323.2 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 293.9 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 235.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 202.0 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 174.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 266.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 80.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 195.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 294.8 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 261.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 173.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 202.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 231.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 173.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 98.0 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 359.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 359.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 228.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 202.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 282.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 293.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 228.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 293.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 80.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 202.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 228.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 269.6 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 235.8 |
BN (mp-984) | <1 0 0> | <0 1 1> | 155.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 326.5 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 235.8 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 293.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 359.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 130.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 161.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 326.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 207.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 121.2 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 1> | 242.0 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 269.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 121.2 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 202.0 |
MoS2 (mp-1434) | <1 0 1> | <0 1 1> | 207.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.07620 | 0.00000 | 0.18023 |
0.20689 | 0.15864 | 0.35900 | 0.00000 | 0.01183 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.18089 | 0.00000 | -0.12026 |
Piezoelectric Modulus ‖eij‖max0.44384 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-1.00000 |
2.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.01 | 0.00 | 0.07 |
0.00 | 3.14 | 0.00 |
0.07 | 0.00 | 3.28 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.72 | 0.00 | 0.15 |
0.00 | 7.62 | 0.00 |
0.15 | 0.00 | 8.44 |
Polycrystalline dielectric constant
εpoly∞
3.14
|
Polycrystalline dielectric constant
εpoly
7.93
|
Refractive Index n1.77 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.3892 | 0.023 | 3 |
Co5(P3O11)2 (mp-31617) | 0.4404 | 0.034 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3349 | 0.082 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4239 | 0.028 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.3972 | 0.038 | 3 |
LiVP2O7 (mp-18911) | 0.0799 | 0.033 | 4 |
LiCrP2O7 (mp-19103) | 0.0984 | 0.000 | 4 |
LiScP2O7 (mp-10517) | 0.1195 | 0.000 | 4 |
LiTiP2O7 (mp-26629) | 0.1728 | 0.055 | 4 |
LiCoP2O7 (mp-31535) | 0.1683 | 0.057 | 4 |
FeO2 (mvc-11999) | 0.7375 | 0.372 | 2 |
Li2VFe(P2O7)2 (mp-764318) | 0.1084 | 0.000 | 5 |
Li2VFe(P2O7)2 (mp-764299) | 0.0943 | 0.000 | 5 |
Li2MnV(P2O7)2 (mp-779885) | 0.1078 | 0.017 | 5 |
Li2VFe(P2O7)2 (mp-763852) | 0.0943 | 0.003 | 5 |
Li2MnV(P2O7)2 (mp-764603) | 0.0975 | 0.018 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5528 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5231 | 0.330 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5647 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.9604 eV |
Corrected Energy-168.4260 eV
-168.4260 eV = -153.1279 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)