material

TiFeO3

ID:

mp-19417

DOI:

10.17188/1194428


Tags: Iron titanium(IV) trioxide Ilmenite Iron(II) titanate(IV) Iron titanate(IV) Iron titanium oxide Iron titanum oxide High pressure experimental phase Iron titanate Iron(III) trioxotitanate(III)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-2.718 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.63 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiFeO3
Band Gap
2.020 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 9805 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 301.0
AlN (mp-661) <0 0 1> <0 0 1> 162.1
AlN (mp-661) <1 0 0> <0 0 1> 208.4
AlN (mp-661) <1 0 1> <1 0 1> 306.1
AlN (mp-661) <1 1 0> <0 0 1> 138.9
AlN (mp-661) <1 1 1> <1 1 1> 256.9
CeO2 (mp-20194) <1 1 0> <0 0 1> 347.4
GaAs (mp-2534) <1 1 1> <0 0 1> 162.1
CeO2 (mp-20194) <1 1 1> <0 0 1> 162.1
BaF2 (mp-1029) <1 1 1> <0 0 1> 69.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 115.8
BaF2 (mp-1029) <1 1 0> <1 0 0> 218.8
GaN (mp-804) <1 1 0> <1 0 0> 145.9
GaN (mp-804) <0 0 1> <0 0 1> 277.9
GaN (mp-804) <1 0 0> <1 0 1> 153.1
GaN (mp-804) <1 0 1> <0 0 1> 324.2
SiO2 (mp-6930) <0 0 1> <0 0 1> 23.2
SiO2 (mp-6930) <1 0 0> <0 0 1> 138.9
SiO2 (mp-6930) <1 0 1> <1 0 0> 72.9
SiO2 (mp-6930) <1 1 1> <0 0 1> 162.1
KCl (mp-23193) <1 0 0> <0 0 1> 208.4
KCl (mp-23193) <1 1 0> <0 0 1> 277.9
KCl (mp-23193) <1 1 1> <0 0 1> 69.5
InAs (mp-20305) <1 0 0> <0 0 1> 115.8
InAs (mp-20305) <1 1 0> <1 0 0> 218.8
ZnSe (mp-1190) <1 1 1> <0 0 1> 162.1
InAs (mp-20305) <1 1 1> <0 0 1> 69.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 208.4
CdS (mp-672) <1 0 1> <1 0 1> 229.6
CdS (mp-672) <0 0 1> <0 0 1> 208.4
LiF (mp-1138) <1 0 0> <1 1 0> 252.7
LiF (mp-1138) <1 1 1> <0 0 1> 208.4
Te2W (mp-22693) <0 1 0> <1 0 0> 218.8
Te2W (mp-22693) <1 1 0> <1 0 0> 218.8
TePb (mp-19717) <1 1 1> <0 0 1> 301.0
Te2Mo (mp-602) <0 0 1> <0 0 1> 208.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 277.9
Ag (mp-124) <1 1 0> <0 0 1> 370.5
Ag (mp-124) <1 1 1> <0 0 1> 92.6
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 69.5
Te2Mo (mp-602) <1 0 0> <1 0 0> 218.8
Ag (mp-124) <1 0 0> <1 0 0> 291.8
BN (mp-984) <0 0 1> <1 0 0> 218.8
BN (mp-984) <1 0 1> <0 0 1> 162.1
GaSe (mp-1943) <0 0 1> <0 0 1> 92.6
BN (mp-984) <1 0 0> <0 0 1> 162.1
BN (mp-984) <1 1 0> <0 0 1> 69.5
BN (mp-984) <1 1 1> <1 0 1> 229.6
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 23.2
LiNbO3 (mp-3731) <1 1 1> <1 1 1> 128.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
291 156 100 11 5 0
156 291 100 -11 -5 0
100 100 231 0 0 0
11 -11 0 27 0 -5
5 -5 0 0 27 11
0 0 0 -5 11 67
Compliance Tensor Sij (10-12Pa-1)
5.4 -2.7 -1.2 -3.5 -1.4 -0.0
-2.7 5.4 -1.2 3.5 1.4 -0.0
-1.2 -1.2 5.4 -0.0 -0.0 0.0
-3.5 3.5 -0.0 41.0 -0.0 2.8
-1.4 1.4 0.0 -0.0 41.0 -7.0
-0.0 -0.0 0.0 2.8 -7.0 16.2
Shear Modulus GV
55 GPa
Bulk Modulus KV
169 GPa
Shear Modulus GR
40 GPa
Bulk Modulus KR
163 GPa
Shear Modulus GVRH
47 GPa
Bulk Modulus KVRH
166 GPa
Elastic Anisotropy
1.95
Poisson's Ratio
0.37

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.06 -0.00 -0.00
0.00 6.06 0.00
-0.00 0.00 5.34
Dielectric Tensor εij (total)
24.58 -0.00 -0.00
0.00 24.58 0.00
-0.00 0.00 17.45
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.82
Polycrystalline dielectric constant εpoly
(total)
22.20
Refractive Index n
2.41
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiCoO3 (mp-19424) 0.1019 0.003 3
TiCoO3 (mp-558233) 0.1053 0.003 3
MgTiO3 (mp-3771) 0.1166 0.000 3
TiFeO3 (mp-818838) 0.0053 0.012 3
TiZnO3 (mp-14142) 0.1773 0.028 3
Li3Nb4NiO12 (mp-772009) 0.2794 0.080 4
Li3Nb4FeO12 (mp-771984) 0.3106 0.051 4
Mg2VWO6 (mvc-5881) 0.3266 0.022 4
Mg2TiWO6 (mvc-5939) 0.3166 0.125 4
InNi2SbO6 (mp-1078367) 0.2724 0.000 4
In2S3 (mp-22375) 0.3477 0.023 2
Sc2O3 (mp-755313) 0.3350 0.039 2
Ga2O3 (mp-1243) 0.3249 0.030 2
In2O3 (mp-22323) 0.3478 0.029 2
Fe2O3 (mp-796253) 0.3483 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.5201 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.6258 0.080 5
Li4MnV2WO12 (mp-773239) 0.6628 0.090 5
Li4Mn2TeWO12 (mp-768044) 0.6018 0.058 5
Li4V2CrTeO12 (mp-775632) 0.6552 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Ti_pv Fe_pv O
Final Energy/Atom
-8.0962 eV
Corrected Energy
-179.1910 eV
Uncorrected energy = -161.9230 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV Corrected energy = -179.1910 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 153493
  • 153492
  • 24790
  • 29209
  • 187688
  • 247547
  • 153673
  • 30671
  • 30670
  • 30672
  • 153674
  • 43466
  • 30669
  • 9805
  • 30665
  • 30667
  • 30666
  • 30668
  • 153494
  • 153491
  • 30673
  • 30664
  • 67046
Submitted by
User remarks:
  • Iron titanate
  • Ilmenite
  • High pressure experimental phase

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)