Final Magnetic Moment7.413 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.140 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/m [10] |
Hall-P 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 220.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 146.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 205.8 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 220.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 274.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 282.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 220.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 274.0 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 293.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 274.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 274.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 -1> | 293.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 274.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 282.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 274.0 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 282.3 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 274.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 219.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 274.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 70.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 274.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 219.2 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 146.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 219.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 274.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 274.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 293.3 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 293.3 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 274.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 219.2 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 219.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 220.0 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 220.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 274.0 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 282.3 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 274.0 |
GaP (mp-2490) | <1 1 0> | <1 0 -1> | 293.3 |
GaP (mp-2490) | <1 0 0> | <1 0 -1> | 146.6 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 -1> | 220.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 274.0 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 -1> | 220.0 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 -1> | 293.3 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 1> | 205.8 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 1> | 205.8 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 219.2 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 274.0 |
Si (mp-149) | <1 0 0> | <1 0 -1> | 146.6 |
Au (mp-81) | <1 1 0> | <0 0 1> | 274.0 |
Si (mp-149) | <1 1 0> | <1 0 1> | 205.8 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 274.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3(W3O8)4 (mp-780475) | 0.6522 | 0.031 | 3 |
BaTa6O16 (mp-769349) | 0.6577 | 0.000 | 3 |
Ta2WO8 (mp-773933) | 0.3337 | 0.003 | 3 |
K2Mo7O20 (mp-579220) | 0.6631 | 0.006 | 3 |
Nb6CdO16 (mp-773090) | 0.6206 | 0.049 | 3 |
U2O5 (mp-647814) | 0.5415 | 0.017 | 2 |
U13O34 (mp-642328) | 0.7054 | 0.017 | 2 |
W8O21 (mp-579377) | 0.2262 | 0.000 | 2 |
W18O49 (mp-567091) | 0.0092 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: W_pv O |
Final Energy/Atom-7.5577 eV |
Corrected Energy-619.0966 eV
-619.0966 eV = -506.3664 eV (uncorrected energy) - 78.3180 eV (MP Advanced Correction) - 34.4122 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)