Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-3.016 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.150 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToU3O8 + Cr2O3 + UO2 |
Band Gap0.542 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 176.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 227.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 50.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 126.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 247.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 278.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 278.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 278.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 278.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 202.5 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 200.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 200.8 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 227.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 202.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 278.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 151.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 200.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 278.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 354.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 202.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 253.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 200.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 133.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 191.7 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 278.5 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 278.5 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 293.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 227.8 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 234.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 319.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 185.9 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 309.8 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 0> | 256.0 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 267.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 151.9 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 319.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 75.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 177.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 253.2 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 227.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 278.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 227.8 |
C (mp-66) | <1 0 0> | <1 1 0> | 256.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 75.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 177.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 354.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 309.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 177.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 177.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 191.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TaAlO4 (mp-8898) | 0.1248 | 0.020 | 3 |
AlTeO4 (mp-752394) | 0.1095 | 0.053 | 3 |
HfCrO4 (mp-781615) | 0.1124 | 0.061 | 3 |
UFeO4 (mp-540677) | 0.0572 | 0.360 | 3 |
UCrO4 (mp-618350) | 0.0347 | 0.150 | 3 |
LiMnFeF6 (mp-555001) | 0.1959 | 0.003 | 4 |
LiFe7(O3F5)2 (mp-777195) | 0.2024 | 0.107 | 4 |
LiMnFeF6 (mp-566418) | 0.1588 | 0.000 | 4 |
LiMnFeF6 (mp-648400) | 0.1970 | 0.003 | 4 |
LiTiMnF6 (mp-556715) | 0.2141 | 0.027 | 4 |
TiO2 (mp-775938) | 0.2624 | 0.039 | 2 |
Rb2O (mp-755459) | 0.2624 | 0.018 | 2 |
CaCl2 (mp-571642) | 0.2197 | 0.001 | 2 |
SiO2 (mp-32667) | 0.2376 | 0.241 | 2 |
Co2N (mp-22631) | 0.2505 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: U Cr_pv O |
Final Energy/Atom-9.0017 eV |
Corrected Energy-235.0289 eV
Uncorrected energy = -216.0409 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.999 eV/atom x 4.0 atoms) = -7.9960 eV
Corrected energy = -235.0289 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)