Final Magnetic Moment0.993 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.895 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaFe(SiO3)2 + Li2Si2O5 + Na2Si2O5 + SiO2 |
Band Gap3.392 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 146.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 146.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 146.0 |
Au (mp-81) | <1 1 0> | <0 1 0> | 146.0 |
Au (mp-81) | <1 1 1> | <1 0 0> | 179.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 146.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 179.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <0 1 0> | 146.0 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 0> | 179.5 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 179.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Fe(Si2O5)3 (mp-851041) | 0.4762 | 0.068 | 4 |
Li2Cr(Si2O5)3 (mp-775349) | 0.5612 | 0.033 | 4 |
Na2Mg2(Si2O5)3 (mp-12187) | 0.3952 | 0.004 | 4 |
Na3Dy(Si2O5)3 (mp-555604) | 0.6033 | 0.000 | 4 |
Na3Y(Si2O5)3 (mp-14977) | 0.6262 | 0.007 | 4 |
NaLiZr(Si2O5)3 (mp-15543) | 0.6790 | 0.000 | 5 |
Na2LiY(Si2O5)3 (mp-14030) | 0.4663 | 0.000 | 5 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.7283 | 0.028 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Fe_pv Si O |
Final Energy/Atom-7.1548 eV |
Corrected Energy-768.5462 eV
-768.5462 eV = -715.4768 eV (uncorrected energy) - 42.1374 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)