Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.474 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.981 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 314.2 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 269.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 67.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 134.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 314.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 209.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 127.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 296.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 161.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 172.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 127.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 169.7 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 161.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 127.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 134.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 67.4 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 67.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 212.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 254.5 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 202.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 269.6 |
BN (mp-984) | <0 0 1> | <0 1 1> | 269.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 169.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 254.5 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 259.1 |
LiNbO3 (mp-3731) | <1 1 1> | <1 1 0> | 259.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 212.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 127.3 |
Al (mp-134) | <1 1 0> | <0 1 1> | 67.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 242.2 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 86.4 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 314.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 127.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 209.5 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 157.1 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 209.5 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 157.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 212.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 137.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 1 0> | 259.1 |
LiTaO3 (mp-3666) | <1 1 1> | <1 1 0> | 259.1 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 1> | 202.2 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 202.2 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 86.4 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 209.5 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 52.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 209.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 1> | 161.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 314.2 |
C (mp-66) | <1 1 0> | <1 0 1> | 161.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaSO4 (mp-3164) | 0.2529 | 0.000 | 3 |
RbMnO4 (mp-19678) | 0.2103 | 0.000 | 3 |
KMnO4 (mp-19046) | 0.1855 | 0.007 | 3 |
KGaH4 (mp-696983) | 0.1663 | 0.000 | 3 |
BaBeF4 (mp-12431) | 0.1595 | 0.000 | 3 |
PH2NO2 (mp-696678) | 0.5318 | 1.778 | 4 |
KP(HO)2 (mp-642648) | 0.5413 | 0.000 | 4 |
RbP(HO)2 (mp-24212) | 0.5584 | 0.000 | 4 |
CsOsNO3 (mp-561383) | 0.4630 | 0.000 | 4 |
KPr(SO4)2 (mp-554057) | 0.4949 | 0.000 | 4 |
Si3Cl8 (mp-27189) | 0.6457 | 0.016 | 2 |
SiBr2 (mp-504902) | 0.6103 | 0.039 | 2 |
SiI2 (mp-541053) | 0.5918 | 0.026 | 2 |
CuCl4 (mp-32829) | 0.6476 | 0.099 | 2 |
CBr4 (mp-680422) | 0.6459 | 0.210 | 2 |
KBiS(ClO2)2 (mp-23645) | 0.6629 | 0.000 | 5 |
H24C8S(NO2)2 (mp-707249) | 0.7489 | 0.143 | 5 |
CaGdTh(PO4)3 (mp-695308) | 0.7318 | 0.013 | 5 |
H12C4NClO4 (mp-24767) | 0.7228 | 0.554 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ba_sv Cr_pv O |
Final Energy/Atom-6.8975 eV |
Corrected Energy-184.5275 eV
Uncorrected energy = -165.5395 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.999 eV/atom x 4.0 atoms) = -7.9960 eV
Corrected energy = -184.5275 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)