material

In2HgTe4

ID:

mp-19765

DOI:

10.17188/1194970


Tags: Mercury indium telluride (1/2/4) Mercury diindium telluride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.294 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.97 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.016 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4 [82]
Hall
I 4
Point Group
4
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 25652 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <1 0 1> <1 1 1> 0.006 244.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.006 163.1
KCl (mp-23193) <1 0 0> <0 0 1> 0.008 41.1
MgO (mp-1265) <1 1 0> <1 1 0> 0.009 230.7
KCl (mp-23193) <1 1 0> <1 1 0> 0.010 115.4
GaN (mp-804) <0 0 1> <0 0 1> 0.014 287.9
MoS2 (mp-1434) <1 0 1> <1 0 1> 0.014 274.1
MoS2 (mp-1434) <1 0 0> <1 0 1> 0.014 274.1
WS2 (mp-224) <1 0 0> <1 0 1> 0.017 91.4
Al (mp-134) <1 0 0> <0 0 1> 0.018 82.3
NaCl (mp-22862) <1 0 0> <1 0 0> 0.018 163.1
ZnO (mp-2133) <0 0 1> <0 0 1> 0.020 329.1
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.020 163.1
SiC (mp-8062) <1 0 0> <0 0 1> 0.020 329.1
NdGaO3 (mp-3196) <1 1 1> <1 0 1> 0.022 274.1
C (mp-66) <1 0 0> <0 0 1> 0.023 164.5
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.031 329.1
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.038 82.3
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.040 163.1
Mg (mp-153) <0 0 1> <1 0 0> 0.040 244.7
LiF (mp-1138) <1 0 0> <0 0 1> 0.044 82.3
PbS (mp-21276) <1 0 0> <0 0 1> 0.050 329.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.058 244.7
GaAs (mp-2534) <1 0 0> <1 0 0> 0.058 163.1
WS2 (mp-224) <0 0 1> <1 0 0> 0.059 244.7
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.060 244.9
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.064 205.7
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.065 115.4
SrTiO3 (mp-4651) <1 1 1> <1 0 1> 0.072 274.1
Ni (mp-23) <1 0 0> <0 0 1> 0.073 205.7
Cu (mp-30) <1 0 0> <0 0 1> 0.075 205.7
Ni (mp-23) <1 1 0> <0 0 1> 0.077 329.1
YVO4 (mp-19133) <1 0 0> <1 0 1> 0.079 91.4
BN (mp-984) <1 0 0> <1 0 1> 0.083 274.1
C (mp-48) <1 0 0> <1 0 1> 0.094 274.1
Ge (mp-32) <1 0 0> <1 0 0> 0.097 163.1
CdS (mp-672) <1 1 1> <0 0 1> 0.103 205.7
YVO4 (mp-19133) <1 0 1> <1 0 1> 0.107 274.1
GaN (mp-804) <1 0 0> <0 0 1> 0.111 205.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.112 329.1
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.113 329.1
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.127 244.7
CdS (mp-672) <0 0 1> <0 0 1> 0.128 329.1
BN (mp-984) <1 1 0> <1 0 1> 0.133 274.1
GaTe (mp-542812) <0 0 1> <1 1 0> 0.140 230.7
GaTe (mp-542812) <1 0 -1> <1 1 0> 0.142 230.7
Te2W (mp-22693) <1 0 1> <0 0 1> 0.150 205.7
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.152 287.9
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.154 329.1
AlN (mp-661) <0 0 1> <0 0 1> 0.154 205.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
29 13 16 0 0 -0
13 29 16 0 0 0
16 16 33 0 0 0
0 0 0 16 0 0
0 0 0 0 16 0
-0 0 0 0 0 17
Compliance Tensor Sij (10-12Pa-1)
50.9 -14.6 -17.2 0 0 0.2
-14.6 50.9 -17.2 0 0 -0.2
-17.2 -17.2 46.6 0 0 0
0 0 0 60.8 0 0
0 0 0 0 60.8 0
0.2 -0.2 0 0 0 59.3
Shear Modulus GV
13 GPa
Bulk Modulus KV
20 GPa
Shear Modulus GR
11 GPa
Bulk Modulus KR
20 GPa
Shear Modulus GVRH
12 GPa
Bulk Modulus KVRH
20 GPa
Elastic Anisotropy
0.79
Poisson's Ratio
0.25

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.10046 -0.00552 0.00000
0.00000 0.00000 0.00000 0.00552 -0.10046 0.00000
-0.02707 0.02707 0.00000 0.00000 0.00000 -0.14913
Piezoelectric Modulus ‖eijmax
0.15396 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
11.20 0.00 0.00
0.00 11.20 0.00
0.00 0.00 11.01
Dielectric Tensor εij (total)
15.98 0.00 0.00
0.00 15.98 0.00
0.00 0.00 15.46
Polycrystalline dielectric constant εpoly
(electronic contribution)
11.14
Polycrystalline dielectric constant εpoly
(total)
15.81
Refractive Index n
3.34
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mg(InTe2)2 (mp-35777) 0.0568 0.005 3
Cd(InSe2)2 (mp-22304) 0.0859 0.000 3
In2HgSe4 (mp-20731) 0.0887 0.000 3
In5AgTe8 (mp-569813) 0.1060 0.000 3
Cd(InTe2)2 (mp-21374) 0.0460 0.000 3
CaZnSO (mp-7204) 0.4209 0.010 4
ZnAgPS4 (mp-558807) 0.6229 0.000 4
CaFeSO (mp-1078415) 0.4349 0.224 4
ZnCu4(SnSe4)2 (mvc-14983) 0.6506 0.035 4
Ge3As4 (mp-569600) 0.3929 0.041 2
GeAs (mp-9548) 0.5046 0.002 2
As4C3 (mp-568505) 0.1675 0.874 2
Si3As4 (mp-570744) 0.3037 0.059 2
GeP (mp-1095275) 0.4574 0.015 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: In_d Hg Te
Final Energy/Atom
-2.9199 eV
Corrected Energy
-22.1273 eV
Uncorrected energy = -20.4393 eV Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV Corrected energy = -22.1273 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 639056
  • 25652
Submitted by
User remarks:
  • Mercury indium telluride (1/2/4)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)