Final Magnetic Moment0.038 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.335 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPr3In + PrIn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 327.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 218.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 95.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 239.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 27.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 239.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 118.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 191.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 197.0 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 239.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 218.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 218.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 191.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 47.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 68.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 81.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 118.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 354.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 335.6 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 294.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 191.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 354.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 287.6 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 287.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 109.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 197.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 157.6 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 287.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 143.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 136.5 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 275.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 300.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 157.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 191.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 315.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 95.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 54.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 54.6 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 239.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 191.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 95.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 136.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 109.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 118.2 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 220.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 157.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 27.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 118.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 275.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrCoGe (mp-10394) | 0.0250 | 0.136 | 3 |
CoNiSn (mp-20237) | 0.0369 | 0.161 | 3 |
TiGaPt (mp-22662) | 0.0000 | 0.000 | 3 |
MnAlPt (mp-10892) | 0.0328 | 0.422 | 3 |
MnCoGe (mp-20565) | 0.0493 | 0.245 | 3 |
Er2In (mp-877) | 0.0082 | 0.000 | 2 |
Nd2In (mp-21295) | 0.0055 | 0.006 | 2 |
Sm2In (mp-19816) | 0.0099 | 0.000 | 2 |
Tm2In (mp-21486) | 0.0000 | 0.000 | 2 |
Pr2Tl (mp-12600) | 0.0099 | 0.017 | 2 |
Ti (mp-72) | 0.0778 | 0.000 | 1 |
Li (mp-1063005) | 0.3861 | 0.019 | 1 |
Hf (mp-1009460) | 0.0885 | 0.045 | 1 |
Hg (mp-10861) | 0.3605 | 0.003 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 In_d |
Final Energy/Atom-4.4399 eV |
Corrected Energy-26.6394 eV
-26.6394 eV = -26.6394 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)