Final Magnetic Moment0.168 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.201 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.317 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToIn2Se3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 240.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 60.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 315.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 225.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 300.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 225.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 300.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 240.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 240.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 60.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 315.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 225.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 195.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 60.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 225.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 255.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 315.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 105.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 195.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 345.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 270.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 315.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 225.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 285.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 300.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 315.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 225.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 195.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 240.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 315.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 315.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 195.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 240.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 60.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 120.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 300.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 225.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 15.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 345.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 165.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 150.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 255.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 120.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 195.0 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 225.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 345.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 225.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 120.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 120.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 285.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrAgO2 (mp-1096875) | 0.4751 | 0.092 | 3 |
FeAgO2 (mp-1096980) | 0.4955 | 0.164 | 3 |
NaMnTe2 (mp-12682) | 0.5183 | 0.517 | 3 |
GaAgO2 (mp-1096976) | 0.5008 | 0.085 | 3 |
ScAgO2 (mp-1096798) | 0.4948 | 0.108 | 3 |
LiY3WO8 (mp-773224) | 0.6525 | 0.072 | 4 |
Li3V4NiO12 (mp-772005) | 0.6641 | 0.095 | 4 |
Li2TiS2O (mp-769287) | 0.6288 | 0.032 | 4 |
ScAlCO (mp-1080747) | 0.6378 | 0.000 | 4 |
Li3MnV4O12 (mp-771987) | 0.6723 | 0.285 | 4 |
Li4VFe(TeO6)2 (mp-761819) | 0.7328 | 0.060 | 5 |
Li4MnV2WO12 (mp-773239) | 0.6454 | 0.088 | 5 |
Explore more synthesis descriptions for materials of composition In2Se3.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d Se |
Final Energy/Atom-3.3994 eV |
Corrected Energy-16.9971 eV
-16.9971 eV = -16.9971 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)