material

ZrSiTe

ID:

mp-19917

DOI:

10.17188/1195103


Tags: Zirconium silicon telluride (1/1/1) Zirconium silicide telluride (1/1/1) Zirconium silicide(-II) telluride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.800 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.06 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 15572 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.000 27.4
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.001 206.9
LiAlO2 (mp-3427) <1 0 1> <1 1 1> 0.002 214.0
LiNbO3 (mp-3731) <1 0 1> <1 1 0> 0.002 155.1
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.003 155.1
CsI (mp-614603) <1 0 0> <0 0 1> 0.008 123.1
Al (mp-134) <1 1 0> <1 1 0> 0.012 206.9
Ni (mp-23) <1 1 1> <1 0 0> 0.019 256.0
GaN (mp-804) <1 1 0> <1 0 1> 0.021 117.1
InAs (mp-20305) <1 0 0> <0 0 1> 0.022 342.0
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.024 195.2
AlN (mp-661) <1 0 0> <1 1 0> 0.025 155.1
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.028 156.2
KCl (mp-23193) <1 1 0> <1 0 1> 0.030 117.1
GdScO3 (mp-5690) <0 1 1> <1 0 0> 0.031 109.7
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.031 342.0
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.031 109.4
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.036 123.1
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.037 155.1
PbS (mp-21276) <1 1 1> <1 0 1> 0.039 312.3
Ni (mp-23) <1 1 0> <1 0 1> 0.039 156.2
C (mp-48) <1 0 0> <1 1 0> 0.039 155.1
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.041 123.1
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.047 109.7
LiTaO3 (mp-3666) <1 0 1> <1 1 0> 0.052 155.1
MgO (mp-1265) <1 1 0> <1 0 1> 0.053 78.1
Ag (mp-124) <1 1 0> <0 0 1> 0.054 342.0
GaN (mp-804) <1 0 0> <1 1 0> 0.056 51.7
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.057 109.7
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.057 329.1
Mg (mp-153) <1 1 0> <1 0 1> 0.057 117.1
SrTiO3 (mp-4651) <1 0 0> <1 0 1> 0.059 351.4
Ga2O3 (mp-886) <1 1 1> <1 0 0> 0.059 256.0
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.061 214.0
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.061 205.2
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.066 27.4
SiC (mp-11714) <1 0 1> <1 0 0> 0.069 256.0
LiTaO3 (mp-3666) <1 0 0> <1 1 1> 0.071 214.0
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.074 107.0
InSb (mp-20012) <1 0 0> <0 0 1> 0.075 177.8
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.078 164.2
Au (mp-81) <1 1 0> <0 0 1> 0.090 342.0
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.091 109.4
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.092 123.1
CdTe (mp-406) <1 0 0> <0 0 1> 0.094 177.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.101 123.1
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.101 54.7
Ni (mp-23) <1 0 0> <0 0 1> 0.102 109.4
CaF2 (mp-2741) <1 1 0> <1 0 1> 0.102 351.4
DyScO3 (mp-31120) <0 0 1> <1 0 1> 0.105 351.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
166 34 19 0 0 0
34 166 19 0 0 0
19 19 16 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 73
Compliance Tensor Sij (10-12Pa-1)
7 -0.6 -7.5 0 0 0
-0.6 7 -7.5 0 0 0
-7.5 -7.5 80.3 0 0 0
0 0 0 55.3 0 0
0 0 0 0 55.3 0
0 0 0 0 0 13.7
Shear Modulus GV
40 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
16 GPa
Shear Modulus GVRH
29 GPa
Bulk Modulus KVRH
35 GPa
Elastic Anisotropy
8.37
Poisson's Ratio
0.17

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZrGeTe (mp-3208) 0.4439 0.000 3
SmClF (mp-608254) 0.5525 0.239 3
BaCaI4 (mp-753709) 0.7130 0.069 3
HfSiTe (mp-13963) 0.2891 0.000 3
SrMnSb2 (mp-1079721) 0.6806 0.307 3
CeMnSbO (mp-542723) 0.6503 0.108 4
SmMnSbO (mp-510488) 0.6271 0.855 4
NdMnSbO (mp-18755) 0.6388 1.093 4
CeZnSbO (mp-909296) 0.6552 0.022 4
CeZnSbO (mp-22620) 0.6572 0.022 4
VSe (mp-604914) 0.4299 0.122 2
MnSe (mp-604910) 0.4280 0.105 2
CuI (mp-22863) 0.4879 0.013 2
FeSe (mp-1063876) 0.3263 0.000 2
CrSe (mp-604915) 0.4057 0.140 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Si Te
Final Energy/Atom
-6.5050 eV
Corrected Energy
-39.0300 eV
-39.0300 eV = -39.0300 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 15572
  • 25734
  • 74522
  • 652388
Submitted by
User remarks:
  • Zirconium silicide(-II) telluride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)