Final Magnetic Moment4.023 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.170 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.034 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNpSi2 + Np |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 299.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 299.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 299.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 245.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 234.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 182.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 182.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 239.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 287.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 208.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 365.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 130.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 77.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 163.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 182.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 182.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 130.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 234.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 154.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 104.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 239.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 104.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 239.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 163.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 299.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 179.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 232.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 269.5 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 234.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 130.4 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 182.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 287.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 323.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 52.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 269.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 269.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 339.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 77.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 52.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 323.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 287.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 182.6 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 59.9 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 287.0 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 299.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 287.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCuS (mp-766467) | 0.7091 | 0.040 | 3 |
RbBiF3 (mp-677028) | 0.6459 | 0.133 | 3 |
LiBeB (mp-1018783) | 0.6159 | 0.000 | 3 |
ZrNbP (mp-4500) | 0.7056 | 0.000 | 3 |
LiCaSi2 (mp-13916) | 0.7087 | 0.000 | 3 |
LaSi (mp-7083) | 0.3578 | 0.000 | 2 |
MgSi (mp-1073777) | 0.6217 | 0.104 | 2 |
MgSi (mp-1073812) | 0.6296 | 0.172 | 2 |
MgSi (mp-1073795) | 0.4720 | 0.112 | 2 |
LaGe (mp-1084830) | 0.2568 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Np Si |
Final Energy/Atom-9.3552 eV |
Corrected Energy-74.8412 eV
-74.8412 eV = -74.8412 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)