material

HfB2

ID:

mp-1994

DOI:

10.17188/1195124


Tags: High pressure experimental phase Hafnium boride (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.018 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.12 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 30422 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.004 60.1
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.017 197.2
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.019 266.2
TbScO3 (mp-31119) <1 1 1> <1 1 0> 0.022 284.7
InAs (mp-20305) <1 1 1> <0 0 1> 0.030 266.2
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.033 170.8
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.045 55.7
LaF3 (mp-905) <0 0 1> <0 0 1> 0.048 137.4
Cu (mp-30) <1 1 0> <1 0 1> 0.052 55.7
ZnO (mp-2133) <0 0 1> <0 0 1> 0.054 111.6
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.062 94.9
Ge (mp-32) <1 1 0> <1 1 1> 0.065 187.5
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.066 163.1
BN (mp-984) <0 0 1> <0 0 1> 0.067 103.0
DyScO3 (mp-31120) <1 1 1> <1 1 0> 0.069 284.7
Ga2O3 (mp-886) <1 1 -1> <1 0 0> 0.069 241.1
GaAs (mp-2534) <1 1 0> <1 1 1> 0.070 187.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.074 111.6
GdScO3 (mp-5690) <1 1 1> <1 1 0> 0.076 284.7
AlN (mp-661) <1 0 1> <1 0 1> 0.079 125.3
ZnSe (mp-1190) <1 1 0> <1 1 1> 0.094 187.5
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.097 175.3
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.098 219.1
AlN (mp-661) <1 1 1> <1 1 0> 0.105 56.9
MgAl2O4 (mp-3536) <1 1 0> <1 1 1> 0.109 187.5
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.111 94.9
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.115 170.8
Fe2O3 (mp-24972) <1 1 1> <1 0 1> 0.128 125.3
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.131 132.8
InSb (mp-20012) <1 0 0> <1 0 1> 0.137 264.5
Te2W (mp-22693) <0 0 1> <1 0 0> 0.142 21.9
CdTe (mp-406) <1 0 0> <1 0 1> 0.143 264.5
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.145 151.8
ZrO2 (mp-2858) <1 0 0> <1 1 0> 0.152 56.9
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.162 60.1
Al (mp-134) <1 1 1> <0 0 1> 0.162 111.6
AlN (mp-661) <0 0 1> <0 0 1> 0.165 8.6
Ga2O3 (mp-886) <1 1 0> <1 0 1> 0.172 222.7
MoSe2 (mp-1634) <1 0 1> <1 0 1> 0.183 208.8
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.186 94.9
InSb (mp-20012) <1 1 1> <0 0 1> 0.194 77.3
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.194 163.1
GdScO3 (mp-5690) <1 0 0> <1 1 1> 0.216 187.5
GaTe (mp-542812) <0 0 1> <0 0 1> 0.217 300.5
Fe2O3 (mp-24972) <1 1 0> <1 1 0> 0.230 246.7
CdTe (mp-406) <1 1 1> <0 0 1> 0.230 77.3
LaAlO3 (mp-2920) <1 1 0> <1 1 1> 0.241 125.0
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.244 25.8
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.253 94.9
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.256 265.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
594 65 125 0 0 0
65 594 125 0 0 0
125 125 448 0 0 0
0 0 0 262 0 0
0 0 0 0 262 0
0 0 0 0 0 264
Compliance Tensor Sij (10-12Pa-1)
1.8 -0.1 -0.5 0 0 0
-0.1 1.8 -0.5 0 0 0
-0.5 -0.5 2.5 0 0 0
0 0 0 3.8 0 0
0 0 0 0 3.8 0
0 0 0 0 0 3.8
Shear Modulus GV
246 GPa
Bulk Modulus KV
252 GPa
Shear Modulus GR
239 GPa
Bulk Modulus KR
250 GPa
Shear Modulus GVRH
242 GPa
Bulk Modulus KVRH
251 GPa
Elastic Anisotropy
0.15
Poisson's Ratio
0.13

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KHgAs (mp-7420) 0.0142 0.000 3
BaAsPd (mp-9744) 0.0241 0.000 3
BaZnSi (mp-31147) 0.0478 0.000 3
SrAlSi (mp-3698) 0.0332 0.000 3
SrAlGe (mp-13311) 0.0173 0.000 3
AlB2 (mp-944) 0.0663 0.010 2
SrGa2 (mp-182) 0.0083 0.000 2
B2Mo (mp-960) 0.0000 0.156 2
ZrB2 (mp-1472) 0.0423 0.000 2
B2W (mp-10144) 0.0610 0.258 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Commercial powders were used to prepare the ceramic materials: ZrB2 Grade B (H. C. Starck, Germany), mean particle size 2m; HfB2 (Cerac Incorporated, Milwaukee, USA), 325mesh, mean particle size [...]
HfB2 (Cerac, Milwaukee Wisconsin) and SiC (Reade Advanced Materials, East Providence Rhode Island) were used to mix 80-vol.% HfB2 and 20-vol.% SiC. The -SiC was 4555nm powder (reported) with 97.5% [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition HfB2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv B
Final Energy/Atom
-8.7899 eV
Corrected Energy
-26.3696 eV
-26.3696 eV = -26.3696 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 614424
  • 167821
  • 614420
  • 167823
  • 614422
  • 44315
  • 167826
  • 167820
  • 167824
  • 167822
  • 30422
  • 167825
  • 182828
  • 614426
Submitted by
User remarks:
  • Hafnium boride (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)