material

YCuSb2

ID:

mp-19943

DOI:

10.17188/1195128


Tags: Yttrium copper antimonide (1/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.612 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.15 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 153572 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Si (mp-149) <1 0 0> <0 0 1> 0.000 149.5
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.000 149.5
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.006 224.3
LiF (mp-1138) <1 0 0> <0 0 1> 0.008 149.5
SiC (mp-11714) <1 1 0> <1 0 1> 0.011 324.9
BN (mp-984) <1 0 0> <1 0 0> 0.023 212.4
Ni (mp-23) <1 1 1> <0 0 1> 0.031 149.5
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.032 212.4
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.033 169.9
BN (mp-984) <0 0 1> <0 0 1> 0.033 130.8
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.034 212.4
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.037 243.0
GaTe (mp-542812) <0 1 0> <1 1 1> 0.045 188.8
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.053 180.3
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.064 336.5
Cu (mp-30) <1 0 0> <0 0 1> 0.070 168.2
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.084 300.4
DyScO3 (mp-31120) <0 1 1> <1 0 0> 0.086 212.4
Mg (mp-153) <1 1 1> <0 0 1> 0.089 149.5
C (mp-48) <0 0 1> <1 0 0> 0.090 42.5
C (mp-66) <1 0 0> <0 0 1> 0.098 168.2
C (mp-48) <1 1 0> <0 0 1> 0.102 168.2
Ge (mp-32) <1 0 0> <0 0 1> 0.104 168.2
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.107 243.0
TiO2 (mp-390) <1 1 0> <1 0 0> 0.110 212.4
KP(HO2)2 (mp-23959) <1 0 0> <1 0 1> 0.111 232.1
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.111 169.9
GdScO3 (mp-5690) <1 1 1> <1 0 0> 0.113 212.4
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.113 355.2
CaCO3 (mp-3953) <1 1 0> <0 0 1> 0.116 149.5
GaP (mp-2490) <1 0 0> <0 0 1> 0.117 149.5
KP(HO2)2 (mp-23959) <1 0 1> <1 0 1> 0.119 139.3
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.122 355.2
KP(HO2)2 (mp-23959) <1 1 0> <1 0 1> 0.130 139.3
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.134 297.4
SiC (mp-7631) <1 0 1> <1 1 1> 0.136 188.8
SiC (mp-7631) <1 0 0> <0 0 1> 0.139 93.5
Te2Mo (mp-602) <1 0 0> <1 0 1> 0.141 324.9
KP(HO2)2 (mp-23959) <0 1 0> <1 0 1> 0.142 232.1
ZnO (mp-2133) <1 0 0> <1 0 1> 0.145 139.3
SiC (mp-11714) <1 0 0> <1 1 1> 0.151 62.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.154 130.8
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.158 355.2
BN (mp-984) <1 1 1> <0 0 1> 0.163 205.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.164 130.8
Cu (mp-30) <1 1 0> <1 0 0> 0.167 297.4
LiGaO2 (mp-5854) <0 1 0> <1 0 1> 0.171 232.1
CsI (mp-614603) <1 0 0> <0 0 1> 0.173 243.0
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.175 212.4
LiGaO2 (mp-5854) <1 0 0> <1 0 1> 0.180 139.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
124 49 54 0 0 0
49 124 54 0 0 0
54 54 82 0 0 0
0 0 0 29 0 0
0 0 0 0 29 0
0 0 0 0 0 46
Compliance Tensor Sij (10-12Pa-1)
11.5 -1.8 -6.4 0 0 0
-1.8 11.5 -6.4 0 0 0
-6.4 -6.4 20.5 0 0 0
0 0 0 34.5 0 0
0 0 0 0 34.5 0
0 0 0 0 0 21.9
Shear Modulus GV
32 GPa
Bulk Modulus KV
71 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
69 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
70 GPa
Elastic Anisotropy
0.48
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
GdCuSb2 (mp-20502) 0.0857 0.000 3
HoCuSb2 (mp-21015) 0.0514 0.003 3
ErCuSb2 (mp-1079261) 0.0532 0.008 3
SmCuSb2 (mp-1080116) 0.1023 0.000 3
DyCuSb2 (mp-20859) 0.0417 0.005 3
KEu(CuTe2)2 (mp-624928) 0.6841 0.017 4
U2Cu2As3O (mp-572929) 0.7367 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Cu_pv Sb
Final Energy/Atom
-5.3180 eV
Corrected Energy
-43.3117 eV
Uncorrected energy = -42.5437 eV Composition-based energy adjustment (-0.192 eV/atom x 4.0 atoms) = -0.7680 eV Corrected energy = -43.3117 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 153572
  • 658224
Submitted by
User remarks:
  • Yttrium copper antimonide (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)