material

CaIn2Cu

ID:

mp-19968

DOI:

10.17188/1195151


Tags: Calcium copper indium (1/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.308 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.07 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CaIn2 + Cu
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 106332 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CaCO3 (mp-3953) <1 0 1> <0 1 0> 0.003 269.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.014 288.5
GaSb (mp-1156) <1 1 1> <1 1 1> 0.015 201.2
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.015 201.2
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.015 201.2
PbSe (mp-2201) <1 1 1> <1 1 1> 0.016 201.2
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.017 265.1
SiC (mp-7631) <0 0 1> <0 0 1> 0.017 288.5
CdSe (mp-2691) <1 1 1> <1 1 1> 0.018 201.2
InSb (mp-20012) <1 0 0> <0 1 1> 0.027 176.1
MgF2 (mp-1249) <0 0 1> <0 1 1> 0.028 176.1
CdSe (mp-2691) <1 1 0> <1 0 0> 0.028 163.5
CdTe (mp-406) <1 0 0> <0 1 1> 0.029 176.1
SiC (mp-8062) <1 1 0> <1 0 0> 0.031 81.7
GaSb (mp-1156) <1 1 0> <1 0 0> 0.033 163.5
C (mp-66) <1 1 0> <1 0 0> 0.033 163.5
TePb (mp-19717) <1 1 0> <1 0 0> 0.034 245.2
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.042 163.5
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.044 240.4
PbSe (mp-2201) <1 1 0> <1 0 0> 0.044 163.5
InAs (mp-20305) <1 1 0> <1 0 0> 0.048 163.5
InP (mp-20351) <1 0 0> <0 1 1> 0.051 176.1
C (mp-66) <1 1 1> <1 1 1> 0.052 201.2
BaF2 (mp-1029) <1 0 0> <0 1 1> 0.060 117.4
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.061 201.2
PbSe (mp-2201) <1 0 0> <0 1 1> 0.064 117.4
GaSe (mp-1943) <0 0 1> <0 1 0> 0.067 100.9
LiF (mp-1138) <1 1 1> <0 1 0> 0.068 201.9
LaAlO3 (mp-2920) <1 1 0> <1 0 0> 0.070 245.2
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.070 201.2
TiO2 (mp-390) <1 0 1> <0 1 0> 0.072 235.5
C (mp-48) <1 0 1> <0 1 0> 0.076 336.5
InAs (mp-20305) <1 1 1> <1 1 1> 0.081 201.2
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 0.086 144.3
GaSb (mp-1156) <1 0 0> <0 1 1> 0.086 117.4
Au (mp-81) <1 0 0> <0 1 1> 0.089 176.1
Cu (mp-30) <1 1 1> <1 1 1> 0.092 201.2
CdTe (mp-406) <1 1 0> <1 0 0> 0.103 245.2
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.105 336.6
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.105 201.2
CdSe (mp-2691) <1 0 0> <0 1 1> 0.108 117.4
GaN (mp-804) <0 0 1> <0 0 1> 0.111 240.4
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.113 245.2
InSb (mp-20012) <1 1 0> <1 0 0> 0.118 245.2
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 0 0> 0.118 163.5
WS2 (mp-224) <0 0 1> <0 0 1> 0.121 240.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.121 240.4
Mg (mp-153) <1 1 1> <0 0 1> 0.126 240.4
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.131 336.6
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.132 168.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
90 19 38 0 0 0
19 82 31 0 0 0
38 31 91 0 0 0
0 0 0 23 0 0
0 0 0 0 47 0
0 0 0 0 0 32
Compliance Tensor Sij (10-12Pa-1)
13.7 -1.2 -5.3 0 0 0
-1.2 14 -4.2 0 0 0
-5.3 -4.2 14.5 0 0 0
0 0 0 43.6 0 0
0 0 0 0 21.4 0
0 0 0 0 0 31.4
Shear Modulus GV
32 GPa
Bulk Modulus KV
49 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
48 GPa
Shear Modulus GVRH
31 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
0.36
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TbIn2Ni (mp-672325) 0.1427 0.000 3
YIn2Ni (mp-22056) 0.0920 0.000 3
CaSn2Ir (mp-11957) 0.1829 0.000 3
CaSn2Rh (mp-11959) 0.1942 0.000 3
DyIn2Ni (mp-1079916) 0.1747 0.000 3
LiYb2InGe2 (mp-977355) 0.7219 0.000 4
Sr2LiInGe2 (mp-571617) 0.7337 0.000 4
LiCa2InGe2 (mp-570850) 0.7139 0.000 4
KSi (mp-1217) 0.6587 0.000 2
MgH2 (mp-23712) 0.6482 0.082 2
YbF3 (mp-22072) 0.6297 0.000 2
KGe (mp-2146) 0.6380 0.041 2
CsSn (mp-571056) 0.6231 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv In_d Cu_pv
Final Energy/Atom
-3.2088 eV
Corrected Energy
-25.6708 eV
Uncorrected energy = -25.6708 eV Corrected energy = -25.6708 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 106332
Submitted by
User remarks:
  • Calcium copper indium (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)