@article{Hery1979, author = "Hery, Y. and Damien, D. and Charvillat, J.P.", title = "Protactinium antimonides: Pa Sb2 and Pa3 Sb4", journal = "Radiochemical and Radioanalytical Letters", year = "1979", volume = "37", pages = "17-26", ASTM_id = "RRALAZ" }