material

ScCuSi

ID:

mp-20083

DOI:

10.17188/1195236


Tags: Scandium copper silicide (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.659 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.009 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.81 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
ScCuSi
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TePb (mp-19717) <1 1 0> <0 0 1> 0.004 182.5
WS2 (mp-224) <1 0 1> <0 1 0> 0.008 230.2
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.013 286.7
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.014 189.8
LiGaO2 (mp-5854) <1 0 1> <1 0 1> 0.016 270.7
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.017 78.2
MgF2 (mp-1249) <1 0 1> <0 1 0> 0.017 316.5
GaSe (mp-1943) <1 0 1> <1 1 0> 0.028 277.5
BN (mp-984) <1 1 0> <1 1 0> 0.037 166.5
Te2W (mp-22693) <1 1 0> <1 1 0> 0.039 111.0
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.041 130.3
CdS (mp-672) <1 0 1> <0 1 1> 0.047 194.1
Fe2O3 (mp-24972) <1 0 1> <1 1 0> 0.053 222.0
Te2W (mp-22693) <1 0 0> <0 1 1> 0.054 194.1
Cu (mp-30) <1 0 0> <1 0 0> 0.054 237.3
LiAlO2 (mp-3427) <1 0 1> <1 0 1> 0.054 216.6
Au (mp-81) <1 1 1> <1 0 1> 0.055 270.7
SiC (mp-11714) <1 0 0> <0 1 1> 0.055 155.3
Ag (mp-124) <1 1 1> <1 0 1> 0.059 270.7
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.061 142.4
GaSe (mp-1943) <1 1 1> <0 0 1> 0.064 234.6
TePb (mp-19717) <1 0 0> <0 0 1> 0.065 130.3
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.065 234.6
Al2O3 (mp-1143) <1 1 0> <1 0 1> 0.066 108.3
SrTiO3 (mp-4651) <0 0 1> <0 1 1> 0.069 155.3
YVO4 (mp-19133) <0 0 1> <0 1 0> 0.076 259.0
SiC (mp-7631) <0 0 1> <0 1 0> 0.080 259.0
SrTiO3 (mp-4651) <1 0 1> <0 1 1> 0.081 271.8
Mg (mp-153) <1 1 0> <0 0 1> 0.081 260.7
BaTiO3 (mp-5986) <1 0 1> <0 1 0> 0.081 115.1
GdScO3 (mp-5690) <1 1 1> <1 0 0> 0.082 142.4
SiC (mp-11714) <0 0 1> <0 1 0> 0.085 259.0
CsI (mp-614603) <1 0 0> <0 1 1> 0.086 310.6
GaSe (mp-1943) <1 1 0> <0 0 1> 0.086 234.6
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.088 142.4
LiGaO2 (mp-5854) <1 1 1> <1 0 0> 0.088 332.2
LiGaO2 (mp-5854) <0 0 1> <1 1 1> 0.088 306.6
TbScO3 (mp-31119) <0 1 0> <1 1 1> 0.090 306.6
AlN (mp-661) <1 1 1> <1 0 0> 0.098 142.4
Te2Mo (mp-602) <0 0 1> <0 1 0> 0.101 230.2
DyScO3 (mp-31120) <0 1 0> <1 1 1> 0.107 306.6
SrTiO3 (mp-4651) <1 1 0> <0 1 1> 0.108 310.6
DyScO3 (mp-31120) <1 0 0> <1 1 1> 0.112 183.9
TbScO3 (mp-31119) <1 0 0> <1 1 1> 0.114 183.9
ZnO (mp-2133) <1 0 1> <0 0 1> 0.116 78.2
GdScO3 (mp-5690) <0 1 1> <0 1 1> 0.118 271.8
KTaO3 (mp-3614) <1 1 0> <0 1 0> 0.119 115.1
ZnTe (mp-2176) <1 1 1> <1 1 0> 0.122 333.0
CdTe (mp-406) <1 0 0> <0 0 1> 0.123 130.3
Al (mp-134) <1 1 0> <0 1 0> 0.126 115.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
201 56 57 0 0 0
56 167 116 0 0 0
57 116 177 0 0 0
0 0 0 88 0 0
0 0 0 0 69 0
0 0 0 0 0 62
Compliance Tensor Sij (10-12Pa-1)
5.6 -1.1 -1.1 0 0 0
-1.1 11.2 -7 0 0 0
-1.1 -7 10.6 0 0 0
0 0 0 11.4 0 0
0 0 0 0 14.4 0
0 0 0 0 0 16.2
Shear Modulus GV
65 GPa
Bulk Modulus KV
111 GPa
Shear Modulus GR
55 GPa
Bulk Modulus KR
111 GPa
Shear Modulus GVRH
60 GPa
Bulk Modulus KVRH
111 GPa
Elastic Anisotropy
0.89
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrMgSn (mp-30780) 0.2962 0.000 3
ScGeRh (mp-1095247) 0.3118 0.005 3
LiCaAs (mp-1095289) 0.3027 0.000 3
LiCaBi (mp-569501) 0.3097 0.000 3
HfCuGe (mp-1095504) 0.3027 0.018 3
LiYb2InGe2 (mp-977355) 0.6987 0.000 4
KNa4SnSb3 (mp-6758) 0.6874 0.005 4
K2BaCdSb2 (mp-863761) 0.6367 0.000 4
K2SrCdSb2 (mp-863758) 0.6894 0.000 4
LiCa2InGe2 (mp-570850) 0.6913 0.000 4
YbH2 (mp-864603) 0.4416 0.000 2
CaH2 (mp-23713) 0.4688 0.000 2
SrH2 (mp-23714) 0.4574 0.000 2
Cs2Se (mp-1011709) 0.4653 0.020 2
BaH2 (mp-23715) 0.4499 0.000 2
Rb (mp-640416) 0.7342 0.057 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Cu_pv Si
Final Energy/Atom
-5.9451 eV
Corrected Energy
-71.3414 eV
-71.3414 eV = -71.3414 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 86391
Submitted by
User remarks:
  • Scandium copper silicide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)